MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Desmopan® 150 Thermoplastic Polyurethane  (discontinued **)
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Desmopan 150 is a TPU on the basis of a standard ester.

Applications: Ski boots, castors, shoe heels, technical injection molding parts.

Information provided by Bayer.

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Key Words: TPUR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.25 g/cc0.0452 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9696DIN 53505
Hardness, Shore D 5050DIN 53505
Elongation at Break >= 50 %>= 50 %Nominal
Compression Set 55 %
@Temperature 70.0 °C
55 %
@Temperature 158 °F
24 hr
 25 %
@Temperature 22.0 °C,
Time 252000 sec
25 %
@Temperature 71.6 °F,
Time 70.0 hour
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm
Surface Resistance 2.00e+12 ohm2.00e+12 ohm
Dielectric Constant  4.6
@Frequency 1e+6 Hz
4.6
@Frequency 1e+6 Hz
 6.0
@Frequency 100 Hz
6.0
@Frequency 100 Hz
Dielectric Strength 14.1 kV/mm358 kV/in
Dissipation Factor  0.029
@Frequency 100 Hz
0.029
@Frequency 100 Hz
 0.066
@Frequency 1e+6 Hz
0.066
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 210 µm/m-°C
@Temperature 20.0 °C
117 µin/in-°F
@Temperature 68.0 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Desmopan® 359 Thermoplastic Polyurethane
Chi Mei Polylac® PA-747 ABS
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade
Covestro Desmopan® 385 Thermoplastic Polyurethane
Covestro Desmopan® 460 Thermoplastic Polyurethane

PBA100 / 26694

Polyurethane

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.