MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to its semicrystalline state. In addition, it displays low outgassing, superior radiation resistance and excellent chemical resistance properties.

Applications:

  • Components for automotive and aircraft engines
  • Transmission
  • Farming, off-road and construction equipment
  • Industrial machinery
  • Electric motors, pumps and compressors
  • Business machines such as laser pointers and high speed copy machines
  • Electronic and semiconductor transport media
  • Analytical and medical equipment
  • Conveyors and textile equipment

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccASTM D792
Water Absorption 0.24 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.10 %24 hours, 23°C, 60% RH
Linear Mold Shrinkage 0.0030 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100ASTM D785
Hardness, Rockwell R 123ASTM D785
Tensile Strength at Break 249.1 MPaASTM D638
Elongation at Break 2.0 %ASTM D638
Flexural Strength 356 MPaASTM D790
Flexural Modulus 20.4 GPaASTM D790
Izod Impact, Notched 12.0 kg-cm/cmASTM D256
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1000 - 10000 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 6.00 µm/m-°C
@Temperature 23.0 °C
MD; ASTM D696
CTE, linear, Transverse to Flow 47.0 µm/m-°C
@Temperature 23.0 °C
ASTM D696
Thermal Conductivity 0.001167 cal cm/sec-cm²-°C
Melting Point 388 °C
Maximum Service Temperature, Air 240 °CHeat distortion temperature, load unknown; ASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 390 - 420 °CInjection molding, extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
Mitsui AURUM® JNF3020 Thermoplastic Polyimide Resin, Wear/Friction Grade

PMIT041 / 53217

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.