MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Mitsui AURUM® JCN6230 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic

Material Notes: AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to its semicrystalline state. In addition, it displays low outgassing, superior radiation resistance and excellent chemical resistance properties.

Applications:

  • Components for automotive and aircraft engines
  • Transmission
  • Farming, off-road and construction equipment
  • Industrial machinery
  • Electric motors, pumps and compressors
  • Business machines such as laser pointers and high speed copy machines
  • Electronic and semiconductor transport media
  • Analytical and medical equipment
  • Conveyors and textile equipment

Information provided by Mitsui.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ASTM D792
Water Absorption 0.24 %0.24 %24 hours; ASTM D570
Moisture Absorption at Equilibrium 0.10 %0.10 %24 hours, 23°C, 60% RH
Linear Mold Shrinkage 0.0030 cm/cm0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100100ASTM D785
Hardness, Rockwell R 123123ASTM D785
Tensile Strength at Break 249.1 MPa36130 psiASTM D638
Elongation at Break 2.0 %2.0 %ASTM D638
Flexural Strength 356 MPa51600 psiASTM D790
Flexural Modulus 20.4 GPa2960 ksiASTM D790
Izod Impact, Notched 1.18 J/cm2.20 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1000 - 10000 ohm1000 - 10000 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.00 µm/m-°C
@Temperature 23.0 °C
3.33 µin/in-°F
@Temperature 73.4 °F
MD; ASTM D696
CTE, linear, Transverse to Flow 47.0 µm/m-°C
@Temperature 23.0 °C
26.1 µin/in-°F
@Temperature 73.4 °F
ASTM D696
Thermal Conductivity 0.4883 W/m-K3.383 BTU-in/hr-ft²-°F
Melting Point 388 °C730 °F
Maximum Service Temperature, Air 240 °C464 °FHeat distortion temperature, load unknown; ASTM D648
 
Processing PropertiesMetricEnglishComments
Processing Temperature 390 - 420 °C734 - 788 °FInjection molding, extrusion

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Kapton® 300HN Polyimide Film, 75 Micron Thickness
CEN® Electronic Material CV Polyimide Film, 1 Mil Thickness
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
Overview of materials for Polyimide
Mitsui AURUM® JNF3020 Thermoplastic Polyimide Resin, Wear/Friction Grade

PMIT041 / 53217

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.