TRA-CAST 3104 is a low viscosity, room temperature cure epoxy casting system developed for high performance production encapsulation and impregnating applications where filling fine intricate free space is required. This medium exotherm, low shrinkage system exhibits excellent flow and wetting characteristics. Its low viscosity allows for void-free filling and self-leveling in casting use, and excellent impregnation of fine wire transformers and coils. Fully cured TRA-CAST 3104 is a durable electrical insulator, dimensionally stable over a wide temperature range, and is resistant to moisture, gases, petroleum lubricants and fuels, salts, many mild acids and alkalis, and other organic and inorganic compounds. Information provided by Tra-Con Inc. |