MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 6K High Strength Carbon
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Fiber Designation: C370S5, Satin weave, 5H

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 49.5 %49.5 %Fiber Volume
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 741 MPa
@Temperature 23.0 °C
107000 psi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Tensile Modulus 54.0 GPa
@Temperature 23.0 °C
7830 ksi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Flexural Yield Strength  518 MPa
@Temperature 90.0 °C
75100 psi
@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D790
 921 MPa
@Temperature 23.0 °C
134000 psi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D790
Flexural Modulus  37.0 GPa
@Temperature 90.0 °C
5370 ksi
@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D790
 41.0 GPa
@Temperature 23.0 °C
5950 ksi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D790
Compressive Yield Strength  350 MPa
@Temperature 90.0 °C
50800 psi
@Temperature 194 °F
0°, Conditioning: 23°C; ASTM D965
 610 MPa
@Temperature 23.0 °C
88500 psi
@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D965
Shear Strength  29.0 MPa
@Temperature 60.0 °C
4210 psi
@Temperature 140 °F
0°, Interlaminar, Conditioning: 60°C-90% RH; ASTM D2344
 36.0 MPa
@Temperature 90.0 °C
5220 psi
@Temperature 194 °F
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
 69.0 MPa
@Temperature 23.0 °C
10000 psi
@Temperature 73.4 °F
0°, Interlaminar, Conditioning: 23°C; ASTM D2344
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F
 
Descriptive Properties
Dry Resin Content (%)42

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon
Goodfellow Carbon/Epoxy Composite Sheet
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
Hexcel® HexPly® EH 84 120°C Curing Epoxy Matrix, High Modulus 12k carbon UD tape 110 g/m2

PHEXC196 / 98667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.