MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Goodfellow Carbon/Epoxy Composite Sheet
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: Carbon Fiber - Epoxy Resin Matrix

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 600 MPa87000 psiLongitudinal
 600 MPa87000 psiTransverse
Elongation at Break 0.85 %0.85 %Longitudinal - Tensile
 0.85 %0.85 %Transverse - Tensile
 1.8 %1.8 %Shear - In Plane
Modulus of Elasticity 70.0 GPa10200 ksiTransverse
Tensile Modulus 70.0 GPa10200 ksiLongitudinal
Compressive Strain at Break 0.80 %0.80 %Longitudinal
 0.80 %0.80 %Transverse
Compressive Strength 570 MPa82700 psiLongitudinal
 570 MPa82700 psiTransverse
Shear Modulus 5.00 GPa725 ksiIn Plane
Shear Strength 90.0 MPa13100 psi
 
Thermal PropertiesMetricEnglishComments
CTE, linear 2.10 µm/m-°C
@Temperature 20.0 °C
1.17 µin/in-°F
@Temperature 68.0 °F
Longitudinal
CTE, linear, Transverse to Flow 2.10 µm/m-°C
@Temperature 20.0 °C
1.17 µin/in-°F
@Temperature 68.0 °F
 
Descriptive Properties
Volume Fraction Fibers, %50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexMC® C/2000/R1A Carbon Epoxy Molding Composite
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System
Goodfellow Carbon/Epoxy Composite Rod
Goodfellow Carbon/Epoxy Composite Tube
BS 970 080M40 Carbon Steel

PGOODF117 / 42272

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.