MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: 1947 - 38% resin weight with M46J 52.5% fiber volume

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  46.0 MPa
@Temperature 90.0 °C
6670 psi
@Temperature 194 °F
90º, Conditioning: 23°C; ASTM D3039
 50.0 MPa
@Temperature 23.0 °C
7250 psi
@Temperature 73.4 °F
90º, Conditioning: 23°C; ASTM D3039
 1823 MPa
@Temperature 23.0 °C
264400 psi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D3039
Tensile Modulus  5.30 GPa
@Temperature 90.0 °C
769 ksi
@Temperature 194 °F
90º, Conditioning: 23°C; ASTM D3039
 7.60 GPa
@Temperature 23.0 °C
1100 ksi
@Temperature 73.4 °F
90º, Conditioning: 23°C; ASTM D3039
 213 GPa
@Temperature 23.0 °C
30900 ksi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D3039
Flexural Yield Strength  906 MPa
@Temperature 90.0 °C
131000 psi
@Temperature 194 °F
0º, Conditioning: 23°C; ASTM D790
 1120 MPa
@Temperature 23.0 °C
162000 psi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D790
Flexural Modulus  191 GPa
@Temperature 90.0 °C
27700 ksi
@Temperature 194 °F
0º, Conditioning: 23°C; ASTM D790
 199 GPa
@Temperature 23.0 °C
28900 ksi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D790
Compressive Yield Strength 196 MPa28400 psiCompression After Impact @ 6.67 J/mm
 965 MPa
@Temperature 23.0 °C
140000 psi
@Temperature 73.4 °F
0º, 120°C Cure, Conditioning: 23°C; ASTM D965
 1052 MPa
@Temperature 23.0 °C
152600 psi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D965
Shear Strength  46.0 MPa
@Temperature 60.0 °C
6670 psi
@Temperature 140 °F
0º Interlaminar Shear, Conditioning: 60°C-90%RH; ASTM D2344
 54.0 MPa
@Temperature 90.0 °C
7830 psi
@Temperature 194 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
 58.0 MPa
@Temperature 90.0 °C
8410 psi
@Temperature 194 °F
0º Interlaminar Shear, 120°C Cure, Conditioning: 23°C; ASTM D2344
 80.0 MPa
@Temperature 23.0 °C
11600 psi
@Temperature 73.4 °F
0º Interlaminar Shear, 120°C Cure, Conditioning: 23°C; ASTM D2344
 81.0 MPa
@Temperature 23.0 °C
11700 psi
@Temperature 73.4 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
APCM DA 4518U Unidirectional Carbon Epoxy Prepreg System
Solvay CYCOM® 5250-4 BMI Prepreg System with IM7-6K-5HS Woven Carbon Fiber

PHEXC187 / 98658

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.