MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Woven Carbon Prepreg
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Epoxy; Epoxy/Carbon Fiber Composite

Material Notes: 42% resin weight with C193PW(HTA) - 193 g/m2 plain weave 3K HTA 49% fiber volume

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 920 MPa
@Temperature 23.0 °C
133000 psi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D3039
Tensile Modulus 60.0 GPa
@Temperature 23.0 °C
8700 ksi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D3039
Flexural Yield Strength  935 MPa
@Temperature 90.0 °C
136000 psi
@Temperature 194 °F
0º, Conditioning: 23°C; ASTM D790
 950 MPa
@Temperature 23.0 °C
138000 psi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D790
Flexural Modulus  40.0 GPa
@Temperature 90.0 °C
5800 ksi
@Temperature 194 °F
0º, Conditioning: 23°C; ASTM D790
 43.0 GPa
@Temperature 23.0 °C
6240 ksi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D790
Compressive Yield Strength  537 MPa
@Temperature 90.0 °C
77900 psi
@Temperature 194 °F
0º, Conditioning: 23°C; ASTM D965
 715 MPa
@Temperature 23.0 °C
104000 psi
@Temperature 73.4 °F
0º, Conditioning: 23°C; ASTM D965
Shear Strength  39.0 MPa
@Temperature 60.0 °C
5660 psi
@Temperature 140 °F
0º Interlaminar Shear, Conditioning: 60°C-90%RH; ASTM D2344
 57.0 MPa
@Temperature 90.0 °C
8270 psi
@Temperature 194 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
 80.0 MPa
@Temperature 23.0 °C
11600 psi
@Temperature 73.4 °F
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 - 130 °C248 - 266 °FEpoxy Matrix Limit
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month
@Temperature -18.0 °C
12.0 Month
@Temperature -0.400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
APCM DA 409U/G35 150 Unidirectional Carbon Epoxy Prepreg System
APCM DA 4518U Unidirectional Carbon Epoxy Prepreg System
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg M46J Fibre
Solvay CYCOM® 5250-4 BMI Prepreg System with IM7-6K-5HS Woven Carbon Fiber
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre

PHEXC186 / 98657

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.