MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem PN2021 EVA Foam Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: PN2021 is an Ethylene-Vinyl Acetate (EVA) copolymer mainly used for the production of crosslinked/expanded plates and other parts. It is a product with easy processability and high compatibility with mineral fillers and other thermoplastics and elastomers. Other important characteristics are elasticity, flexibility, excellent stress cracking resistance (ESCR), chemical resistance, and low temperature strength. The exclusive morphologic characteristics give crosslinkability. The components produced with PN2021 have the following properties: lightness, resistance to deformation, low shrink, high capacity of sticking, and retention of colors. It contains antioxidant additives. Its applications include: shoe components (soles, insoles, etc.); expanded and/or cross linked artifacts for toys, games, floats, advertising, and office materials; tubing and profiles; and polymeric blends.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM-D1505
Vinyl Acetate Content 19 %19 %
Melt Flow 2.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8989ASTM-D2240
Hardness, Shore D 3838ASTM-D2240
Tensile Strength at Break 19.0 MPa2760 psiASTM-D638
Elongation at Break 750 %750 %ASTM-D638
Secant Modulus 0.0330 GPa4.79 ksi5%; ASTM-D638
 
Thermal PropertiesMetricEnglishComments
Melting Point 86.0 °C187 °FASTM-D3418
Vicat Softening Point 61.0 °C
@Load 1.02 kg
142 °F
@Load 2.25 lb
ASTM-D1525
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 90.0 °C176 - 194 °FHomogenization (Calendering)
 100 - 120 °C212 - 248 °FMixing (Bambury)
 160 - 175 °C320 - 347 °FPressing
 
Descriptive Properties
Pressing Pressure (kgf/cm²)100minimum

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem Evateno® 3019 PE EVA Foam Copolymer
Braskem VA2019A EVA Foam Copolymer
Braskem Evateno® 8019 PE EVA Foam Copolymer
Braskem Evateno® HM 150 EVA Hot Melt Copolymer
Braskem Evateno® HM 2528 EVA Hot Melt Copolymer

PBRAS820 / 106666

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.