MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem VA2019A EVA Foam Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate

Material Notes: The VA2019A is a copolymer of Ethylene-Vinyl Acetate (EVA) with medium vinyl-acetate content. VA2019A is an easy processing product with high compatibility with other thermoplastic and elastomeric resins and mineral loads. Its elasticity is higher than the LDPE of the same MI. It has excellent environmental stress crack resistance (ESCR) and low temperature brittleness. The compounds produced with VA2019A will have lightness, good resistance to deformation, and high retention of color. Crosslinked and/or expanded parts have several applications including: compounds for the footwear (sole, insoles, etc), toys, and gifts industry (produced by injection molding); and polymeric blends.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³ASTM-D1505 / ASTM-D792
ESCR 100% Igepal® >= 300 hour
@Thickness 2.00 mm,
Temperature 50.0 °C
>= 300 hour
@Thickness 0.0787 in,
Temperature 122 °F
0.3 mm notched-plaques; ASTM-D1693
Vinyl Acetate Content 18 %18 %
Melt Flow 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090ASTM-D2240
Hardness, Shore D 3131ASTM-D2240
 
Thermal PropertiesMetricEnglishComments
Melting Point 87.0 °C189 °FASTM-D3418
Vicat Softening Point 62.0 °C
@Load 1.02 kg
144 °F
@Load 2.25 lb
ASTM-D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem PN2021 EVA Foam Copolymer
Braskem Evateno® 8019 PE EVA Foam Copolymer
Braskem Evateno® 3019 PE EVA Foam Copolymer
Petroquimica Triunfo Tritheva® PN 2021 EVA Copolymer
Arkema OREVAC® 18211 Maleic Anhydride Grafted EVA Copolymer

PBRAS821 / 106667

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.