MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
5754-H26 Aluminum
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes:
Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A95754; Aluminium 5754; AA5754-H26; Al5754-H26
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.67 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 85
Tensile Strength, Ultimate 290 MPa
Tensile Strength, Yield 245 MPa0.2% offset
Elongation at Break 10 %
Modulus of Elasticity 70.3 GPaAA5154; Average of tension and compression
Poissons Ratio 0.33AA5154
Shear Modulus 25.9 GPaAA5154
Shear Strength 170 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000532 ohm-cmAA5154
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.9 µm/m-°C
@Temperature 20.0 - 100 °C
AA5154
Specific Heat Capacity 0.900 J/g-°CAA5154
Thermal Conductivity 125 W/m-KAA5154
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 93.6 - 97.3 %As remainder
Chromium, Cr <= 0.30 %
Copper, Cu <= 0.10 %
Cr + Mn 0.10 - 0.60 %
Iron, Fe <= 0.40 %
Magnesium, Mg 2.6 - 3.6 %
Manganese, Mn <= 0.50 %
Other, each <= 0.050 %
Other, total <= 0.15 %
Silicon, Si <= 0.40 %
Titanium, Ti <= 0.15 %
Zinc, Zn <= 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
5754-H22 Aluminum
5754-H24 Aluminum
Constellium PLAN OX 5754 Aluminum Rolled Plate
Constellium PLAN 5754 Aluminum Rolled Plate
Aluminum 5056-H38

MA5754H26 / 130361

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.