MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Constellium PLAN 5754 Aluminum Rolled Plate
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 5000 Series Aluminum Alloy

Material Notes: Rolled plates in 5754 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 5754 PLAN is mainly used for low stressed mechanical components, manufactured by intensive machining. Typical applications include parts for packaging machines.

Information provided by manufacturer

Key Words: EN AW-5754; Al Mg3
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.67 g/cc0.0965 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell  76
@Thickness 20.0 - 150 mm
76
@Thickness 0.787 - 5.91 in
 77
@Thickness 4.00 - 20.0 mm
77
@Thickness 0.157 - 0.787 in
Tensile Strength  190 - 240 MPa
@Thickness 4.00 - 12.5 mm
27600 - 34800 psi
@Thickness 0.157 - 0.492 in
Temper H111; Standard EN 485-2
 >= 255 MPa
@Thickness 12.5 - 100 mm
>= 37000 psi
@Thickness 0.492 - 3.94 in
Temper H111; Standard EN 485-2
 295 MPa
@Thickness 4.00 - 20.0 mm
42800 psi
@Thickness 0.157 - 0.787 in
Typical Strength
 295 MPa
@Thickness 20.0 - 150 mm
42800 psi
@Thickness 0.787 - 5.91 in
Typical Strength
Tensile Strength, Yield  >= 80.0 MPa
@Strain 0.2 %,
Thickness 4.00 - 12.5 mm
>= 11600 psi
@Strain 0.2 %,
Thickness 0.157 - 0.492 in
Temper H111; Standard EN 485-2
 >= 105 MPa
@Strain 0.2 %,
Thickness 12.5 - 100 mm
>= 15200 psi
@Strain 0.2 %,
Thickness 0.492 - 3.94 in
Temper H111; Standard EN 485-2
 140 MPa
@Strain 0.2 %,
Thickness 20.0 - 150 mm
20300 psi
@Strain 0.2 %,
Thickness 0.787 - 5.91 in
Typical Strength
 150 MPa
@Strain 0.2 %,
Thickness 4.00 - 20.0 mm
21800 psi
@Strain 0.2 %,
Thickness 0.157 - 0.787 in
Typical Strength
Elongation at Break  >= 12 %
@Thickness 12.5 - 100 mm
>= 12 %
@Thickness 0.492 - 3.94 in
Temper H111; Standard EN 485-2
 >= 18 %
@Thickness 4.00 - 12.5 mm
>= 18 %
@Thickness 0.157 - 0.492 in
Temper H111; Standard EN 485-2
 22 %
@Thickness 20.0 - 150 mm
22 %
@Thickness 0.787 - 5.91 in
Typical Elongation; Standard EN 485-2
 23 %
@Thickness 4.00 - 20.0 mm
23 %
@Thickness 0.157 - 0.787 in
Typical Elongation; Standard EN 485-2
Modulus of Elasticity 70.0 GPa10200 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000400 - 0.00000520 ohm-cm0.00000400 - 0.00000520 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.8 µm/m-°C
@Temperature 20.0 - 100 °C
13.2 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 130 - 140 W/m-K902 - 972 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 94.35 - 97.4 %94.35 - 97.4 %as balance
Chromium, Cr <= 0.30 %<= 0.30 %
Copper, Cu <= 0.10 %<= 0.10 %
Iron, Fe <= 0.40 %<= 0.40 %
Magnesium, Mg 2.6 - 3.6 %2.6 - 3.6 %
Manganese, Mn <= 0.50 %<= 0.50 %
Silicon, Si <= 0.40 %<= 0.40 %
Zinc, Zn <= 0.20 %<= 0.20 %
Zr+Ti <= 0.15 %<= 0.15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Constellium PLAN OX 5754 Aluminum Rolled Plate
5754-H22 Aluminum
5754-H24 Aluminum
5754-H26 Aluminum
Aluminum 5154-O

NCONS003 / 160266

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.