MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

ASTM A229 Oil-tempered Steel Wire, Class II
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Pretempered steel wire used for mechanical springs and wire forms

Key Words: UNS K07001
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1320 - 1490 MPa
@Diameter 15.9 mm
191000 - 216000 psi
@Diameter 0.626 in
 1350 - 1520 MPa
@Diameter 12.7 mm
196000 - 220000 psi
@Diameter 0.500 in
 1420 - 1590 MPa
@Diameter 9.53 mm
206000 - 231000 psi
@Diameter 0.375 in
 1440 - 1610 MPa
@Diameter 7.92 mm
209000 - 234000 psi
@Diameter 0.312 in
 1450 - 1630 MPa
@Diameter 6.35 mm
210000 - 236000 psi
@Diameter 0.250 in
 1490 - 1660 MPa
@Diameter 5.26 mm
216000 - 241000 psi
@Diameter 0.207 in
 1590 - 1770 MPa
@Diameter 4.11 mm
231000 - 257000 psi
@Diameter 0.162 in
 1730 - 1940 MPa
@Diameter 3.05 mm
251000 - 281000 psi
@Diameter 0.120 in
 1830 - 2040 MPa
@Diameter 2.00 mm
265000 - 296000 psi
@Diameter 0.0787 in
 1920 - 2120 MPa
@Diameter 1.60 mm
278000 - 307000 psi
@Diameter 0.0630 in
 1960 - 2160 MPa
@Diameter 1.40 mm
284000 - 313000 psi
@Diameter 0.0551 in
 2050 - 2250 MPa
@Diameter 1.00 mm
297000 - 326000 psi
@Diameter 0.0394 in
 2140 - 2350 MPa
@Diameter 0.810 mm
310000 - 341000 psi
@Diameter 0.0319 in
 2190 - 2390 MPa
@Diameter 0.660 mm
318000 - 347000 psi
@Diameter 0.0260 in
 2230 - 2440 MPa
@Diameter 0.510 mm
323000 - 354000 psi
@Diameter 0.0201 in
Modulus of Elasticity 200 GPa29000 ksiTypical Carbon Steel
Bulk Modulus 160 GPa23200 ksiTypical for Steel
Poissons Ratio 0.290.29Typical Carbon Steel
Shear Modulus 80.0 GPa11600 ksiTypical for Steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FTypical Carbon Steel
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FTypical Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.55 - 0.85 %0.55 - 0.85 %
Iron, Fe 98.29 %98.29 %as balance
Manganese, Mn 0.30 - 1.2 %0.30 - 1.2 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.10 - 0.35 %0.10 - 0.35 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A229 Oil-tempered Steel Wire, Class I
ASTM A227 Steel Wire, Class II
ASTM A228 Steel (UNS K08500)
AISI 1065 Steel, hot rolled, 19-32 mm (0.75-1.25 in) round
ASTM A227 Steel Wire, Class I

MSA229II / 142770

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.