MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A227 Steel Wire, Class I
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Round, hard drawn steel wire for mechanical springs and wire forms

Key Words: UNS K06501
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1010 - 1170 MPa
@Diameter 15.9 mm
147000 - 170000 psi
@Diameter 0.625 in
 1080 - 1240 MPa
@Diameter 12.7 mm
156000 - 180000 psi
@Diameter 0.500 in
 1150 - 1330 MPa
@Diameter 9.52 mm
167000 - 193000 psi
@Diameter 0.375 in
 1250 - 1450 MPa
@Diameter 6.35 mm
182000 - 210000 psi
@Diameter 0.250 in
 1310 - 1500 MPa
@Diameter 5.26 mm
190000 - 218000 psi
@Diameter 0.207 in
 1340 - 1550 MPa
@Diameter 4.50 mm
195000 - 225000 psi
@Diameter 0.177 in
 1400 - 1610 MPa
@Diameter 3.76 mm
203000 - 234000 psi
@Diameter 0.148 in
 1450 - 1660 MPa
@Diameter 3.05 mm
210000 - 241000 psi
@Diameter 0.120 in
 1520 - 1740 MPa
@Diameter 2.34 mm
220000 - 253000 psi
@Diameter 0.0920 in
 1600 - 1830 MPa
@Diameter 1.83 mm
232000 - 266000 psi
@Diameter 0.0720 in
 1680 - 1920 MPa
@Diameter 1.37 mm
243000 - 279000 psi
@Diameter 0.0540 in
 1760 - 2020 MPa
@Diameter 1.04 mm
255000 - 293000 psi
@Diameter 0.0410 in
 1830 - 2110 MPa
@Diameter 0.813 mm
266000 - 306000 psi
@Diameter 0.0320 in
 1900 - 2170 MPa
@Diameter 0.660 mm
275000 - 315000 psi
@Diameter 0.0260 in
 1950 - 2230 MPa
@Diameter 0.508 mm
283000 - 323000 psi
@Diameter 0.0200 in
Modulus of Elasticity 200 GPa29000 ksiTypical Carbon Steel
Bulk Modulus 160 GPa23200 ksiTypical for Steel
Poissons Ratio 0.290.29Typical Carbon Steel
Shear Modulus 80.0 GPa11600 ksiTypical for Steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FTypical Carbon Steel
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FTypical Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.45 - 0.85 %0.45 - 0.85 %may not vary by more than .13% in any one lot
Iron, Fe 98.255 %98.255 %as balance
Manganese, Mn 0.30 - 1.3 %0.30 - 1.3 %may not vary by more than .30% in any one lot
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.050 %<= 0.050 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A227 Steel Wire, Class II
ASTM A228 Steel (UNS K08500)
ASTM A229 Oil-tempered Steel Wire, Class I
ASTM A230 Carbon Steel Wire
ASTM A229 Oil-tempered Steel Wire, Class II

MSA227I / 142765

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.