MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ASTM A229 Oil-tempered Steel Wire, Class I
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; ASTM Steel; Carbon Steel; Medium Carbon Steel

Material Notes: Pretempered steel wire used for mechanical springs and wire forms

Key Words: UNS K07001
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.80 g/cc0.282 lb/in³Typical of ASTM Steel
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  1140 - 1310 MPa
@Diameter 15.9 mm
165000 - 190000 psi
@Diameter 0.626 in
 1170 - 1340 MPa
@Diameter 12.7 mm
170000 - 194000 psi
@Diameter 0.500 in
 1240 - 1410 MPa
@Diameter 9.53 mm
180000 - 205000 psi
@Diameter 0.375 in
 1260 - 1430 MPa
@Diameter 7.92 mm
183000 - 207000 psi
@Diameter 0.312 in
 1280 - 1450 MPa
@Diameter 6.35 mm
186000 - 210000 psi
@Diameter 0.250 in
 1310 - 1480 MPa
@Diameter 5.26 mm
190000 - 215000 psi
@Diameter 0.207 in
 1410 - 1590 MPa
@Diameter 4.11 mm
205000 - 231000 psi
@Diameter 0.162 in
 1520 - 1720 MPa
@Diameter 3.05 mm
220000 - 249000 psi
@Diameter 0.120 in
 1620 - 1830 MPa
@Diameter 2.00 mm
235000 - 265000 psi
@Diameter 0.0787 in
 1700 - 1910 MPa
@Diameter 1.60 mm
247000 - 277000 psi
@Diameter 0.0630 in
 1740 - 1950 MPa
@Diameter 1.40 mm
252000 - 283000 psi
@Diameter 0.0551 in
 1830 - 2040 MPa
@Diameter 1.00 mm
265000 - 296000 psi
@Diameter 0.0394 in
 1930 - 2140 MPa
@Diameter 0.810 mm
280000 - 310000 psi
@Diameter 0.0319 in
 1970 - 2180 MPa
@Diameter 0.660 mm
286000 - 316000 psi
@Diameter 0.0260 in
 2020 - 2230 MPa
@Diameter 0.510 mm
293000 - 323000 psi
@Diameter 0.0201 in
Modulus of Elasticity 200 GPa29000 ksiTypical Carbon Steel
Bulk Modulus 160 GPa23200 ksiTypical for Steel
Poissons Ratio 0.290.29Typical Carbon Steel
Shear Modulus 80.0 GPa11600 ksiTypical for Steel
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm0.0000170 ohm-cmTypical Carbon Steel
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.0 µm/m-°C6.67 µin/in-°FTypical Carbon Steel
Specific Heat Capacity 0.470 J/g-°C0.112 BTU/lb-°FTypical Carbon Steel
Thermal Conductivity 52.0 W/m-K361 BTU-in/hr-ft²-°FTypical Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.55 - 0.85 %0.55 - 0.85 %
Iron, Fe 98.29 %98.29 %as balance
Manganese, Mn 0.30 - 1.2 %0.30 - 1.2 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.10 - 0.35 %0.10 - 0.35 %
Sulfur, S <= 0.030 %<= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ASTM A229 Oil-tempered Steel Wire, Class II
ASTM A228 Steel (UNS K08500)
ASTM A227 Steel Wire, Class I
ASTM A227 Steel Wire, Class II
AISI 1065 Steel, cold drawn, spheroidized, annealed, 19-32 mm (0.75-1.25 in) round

MSA229I / 142769

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.