MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 0.140 - 1.36 g/ccAverage value: 1.09 g/cc Grade Count:172
 1.00 - 1.20 g/cc
@Temperature 40.0 - 40.0 °C
Average value: 1.09 g/cc Grade Count:6
Water Absorption 1.08 - 1.50 %Average value: 1.36 % Grade Count:3
Water Vapor Transmission 420 - 3200 g/m²/dayAverage value: 1460 g/m²/day Grade Count:4
 6000 - 9500 g/m²/day
@Temperature 38.0 - 38.0 °C
Average value: 7750 g/m²/day Grade Count:1
Viscosity 50.0 - 4500 cPAverage value: 866 cP Grade Count:21
 100 - 2000 cP
@Temperature 40.0 - 40.0 °C
Average value: 563 cP Grade Count:6
Maximum Moisture Content 0.0200 - 0.0500Average value: 0.0256 Grade Count:16
Thickness 25.4 - 2030 micronsAverage value: 363 microns Grade Count:9
Linear Mold Shrinkage 0.00100 - 0.0450 cm/cmAverage value: 0.00652 cm/cm Grade Count:40
Linear Mold Shrinkage, Transverse 0.000 - 0.0200 cm/cmAverage value: 0.00618 cm/cm Grade Count:11
Melt Flow 10.0 - 54.0 g/10 minAverage value: 19.2 g/10 min Grade Count:11
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 25.0 - 101Average value: 80.9 Grade Count:189
Hardness, Shore D 22.0 - 78.0Average value: 54.2 Grade Count:43
Tensile Strength, Ultimate 0.500 - 170 MPaAverage value: 31.4 MPa Grade Count:211
 10.3421 - 44.2 MPa
@Temperature 80.0 - 121 °C
Average value: 28.9 MPa Grade Count:9
 10.3421 - 44.2 MPa
@Time 259000 - 1.81e+6 sec
Average value: 28.9 MPa Grade Count:9
Tensile Strength, Yield 0.800 - 70.0 MPaAverage value: 21.8 MPa Grade Count:50
Elongation at Break 4.20 - 1000 %Average value: 504 % Grade Count:217
 400 - 650 %
@Temperature 80.0 - 120 °C
Average value: 563 % Grade Count:8
 400 - 650 %
@Time 259000 - 1.94e+6 sec
Average value: 563 % Grade Count:8
Elongation at Yield 320 - 850 %Average value: 528 % Grade Count:18
Modulus of Elasticity 0.00670 - 13.0 GPaAverage value: 3.69 GPa Grade Count:9
Flexural Yield Strength 1.55 - 205 MPaAverage value: 101 MPa Grade Count:6
Flexural Modulus 0.0162 - 12.0 GPaAverage value: 1.76 GPa Grade Count:21
Resilience 30.0 - 65.0Average value: 46.9 Grade Count:18
Rebound 1.00 - 72.0 %Average value: 41.2 % Grade Count:6
Izod Impact, Notched 0.590 - 0.590 J/cm
@Temperature -40.0 - -40.0 °C
Average value: 0.590 J/cm Grade Count:1
 0.590 - 0.590 J/cm
@Thickness 3.17 - 3.17 mm
Average value: 0.590 J/cm Grade Count:1
Izod Impact, Notched (ISO) 17.0 kJ/m² - NBAverage value: 22.3 kJ/m² Grade Count:4
 7.50 - 12.0 kJ/m²
@Temperature -30.0 - -20.0 °C
Average value: 9.47 kJ/m² Grade Count:7
Izod Impact, Unnotched (ISO) 71.0 - 119 kJ/m²Average value: 91.3 kJ/m² Grade Count:3
 60.0 - 69.0 kJ/m²
@Temperature -30.0 - -30.0 °C
Average value: 64.7 kJ/m² Grade Count:3
Charpy Impact, Notched 5.00 J/cm² - NBAverage value: 7.00 J/cm² Grade Count:13
 0.300 J/cm² - NB
@Temperature -30.0 - -30.0 °C
Average value: 7.95 J/cm² Grade Count:13
Coefficient of Friction 0.0110 - 7.40Average value: 2.96 Grade Count:5
Tear Strength 3.00 - 230 kN/mAverage value: 76.0 kN/m Grade Count:177
Graves Tear Strength 47.3 - 245 kN/mAverage value: 104 kN/m Grade Count:9
K Factor (Wear Factor) 40.0 - 100Average value: 63.1 Grade Count:18
Taber Abrasion, mg/1000 Cycles 4.00 - 340Average value: 56.3 Grade Count:35
Compression Set 1.00 - 100 %Average value: 35.3 % Grade Count:68
Tensile Set 5.60 - 70.0 %Average value: 25.2 % Grade Count:11
Torsional Stiffness 22.0 - 472 MPaAverage value: 181 MPa Grade Count:5
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0500 - 5.60e+12 ohm-cmAverage value: 1.40e+12 ohm-cm Grade Count:4
Surface Resistance 1000 - 5.60e+14 ohmAverage value: 1.40e+14 ohm Grade Count:4
Dielectric Constant 3.70 - 6.70Average value: 5.16 Grade Count:4
Dielectric Strength 14.3 - 15.4 kV/mmAverage value: 15.0 kV/mm Grade Count:3
 
Thermal PropertiesOriginal ValueComments
CTE, linear 86.4 - 179 µm/m-°CAverage value: 139 µm/m-°C Grade Count:3
Melting Point 118 - 218 °CAverage value: 158 °C Grade Count:17
Deflection Temperature at 8.0 MPa 50.0 - 85.0 °CAverage value: 73.3 °C Grade Count:3
Vicat Softening Point 46.0 - 200 °CAverage value: 103 °C Grade Count:42
Brittleness Temperature -70.0 - -68.0 °CAverage value: -68.5 °C Grade Count:4
Glass Transition Temp, Tg -76.0 - -10.0 °CAverage value: -41.8 °C Grade Count:48
Flammability, UL94 V-2 - V-0Grade Count:21
Oxygen Index 21.0 - 38.0 %Average value: 29.2 % Grade Count:11
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.49 - 1.50Average value: 1.49 Grade Count:4
Haze 0.000 - 2.00 %Average value: 1.11 % Grade Count:8
Gloss 90.0 %Average value: 90.0 % Grade Count:4
Yellow Index 1.00 %Average value: 1.00 % Grade Count:4
Transmission, Visible 85.0 - 95.0 %Average value: 91.5 % Grade Count:8
 
Processing PropertiesOriginal ValueComments
Processing Temperature 62.8 - 240 °CAverage value: 190 °C Grade Count:34
Nozzle Temperature 175 - 220 °CAverage value: 205 °C Grade Count:6
Adapter Temperature 175 - 216 °CAverage value: 192 °C Grade Count:27
Die Temperature 170 - 225 °CAverage value: 192 °C Grade Count:46
Melt Temperature 135 - 240 °CAverage value: 185 °C Grade Count:55
Head Temperature 170 - 200 °CAverage value: 186 °C Grade Count:9
Mold Temperature 10.0 - 90.0 °CAverage value: 39.9 °C Grade Count:32
Drying Temperature 70.0 - 180 °CAverage value: 95.8 °C Grade Count:33
Moisture Content 0.100 %Average value: 0.100 % Grade Count:3
Dew Point -40.0 - -5.00 °CAverage value: -36.4 °C Grade Count:20
Injection Pressure 8.27 - 138 MPaAverage value: 34.8 MPa Grade Count:4
Cycle Time - Injection 25.0 - 50.0 secAverage value: 39.0 sec Grade Count:3
Cure Time 120 - 1200 minAverage value: 410 min Grade Count:18

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Overview of materials for Polycarbonate/Thermoplastic Polyurethane Blend
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced

O5045 / 78464

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.