MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Master Bond is a leading manufacturer of high performance epoxy adhesives, sealants, coatings, potting/encapsulation compounds and impregnation resins. Our epoxies include one and two part formulations that can be cured at room temperature, with heat or exposure to UV light. Special formulations feature high electrical and/or thermal conductivity and wide service temperature ranges. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.0400 - 1.74 g/cc0.00145 - 0.0629 lb/in³Average value: 1.12 g/cc Grade Count:299
Volatile Organic Compounds (VOC) Content 0.000 - 766 g/l0.000 - 766 g/lAverage value: 117 g/l Grade Count:17
Water Absorption 2.80 - 7.40 %2.80 - 7.40 %Average value: 4.12 % Grade Count:4
Viscosity 0.890 - 8500 cP0.890 - 8500 cPAverage value: 1320 cP Grade Count:204
 1500 - 3000 cP
@Temperature 35.0 - 35.0 °C
1500 - 3000 cP
@Temperature 95.0 - 95.0 °F
Average value: 2380 cP Grade Count:5
Mooney Viscosity 11.0 - 80.011.0 - 80.0Average value: 33.5 Grade Count:103
Thickness 254 - 6100 microns10.0 - 240 milAverage value: 3770 microns Grade Count:10
Linear Mold Shrinkage 0.000100 - 0.0580 cm/cm0.000100 - 0.0580 in/inAverage value: 0.00458 cm/cm Grade Count:138
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 10.0 - 10510.0 - 105Average value: 67.9 Grade Count:624
 75.0 - 75.0
@Temperature -40.0 - -40.0 °C
75.0 - 75.0
@Temperature -40.0 - -40.0 °F
Average value: 75.0 Grade Count:2
Hardness, Shore D 30.0 - 95.030.0 - 95.0Average value: 71.2 Grade Count:164
Hardness, Shore OO 30.0 - 70.030.0 - 70.0Average value: 47.5 Grade Count:4
Tensile Strength, Ultimate 0.138 - 79.3 MPa20.0 - 11500 psiAverage value: 24.6 MPa Grade Count:631
Tensile Strength, Yield 0.345 - 34.5 MPa50.0 - 5000 psiAverage value: 12.9 MPa Grade Count:16
Elongation at Break 0.400 - 1300 %0.400 - 1300 %Average value: 415 % Grade Count:685
Modulus of Elasticity 0.00114 - 3.54 GPa0.165 - 514 ksiAverage value: 1.29 GPa Grade Count:40
Flexural Yield Strength 2.41 - 310 MPa350 - 45000 psiAverage value: 67.2 MPa Grade Count:54
Flexural Modulus 0.0210 - 6.76 GPa3.05 - 980 ksiAverage value: 1.71 GPa Grade Count:120
 0.0170 - 1.79264 GPa
@Temperature -30.0 - 70.0 °C
2.47 - 260.004 ksi
@Temperature -22.0 - 158 °F
Average value: 0.599 GPa Grade Count:5
Compressive Yield Strength 0.0145 - 82.7 MPa2.10 - 12000 psiAverage value: 41.0 MPa Grade Count:30
Compressive Modulus 0.0283 - 4.76 GPa4.10 - 690 ksiAverage value: 1.26 GPa Grade Count:27
Resilience 4.50 - 50.04.50 - 50.0Average value: 29.2 Grade Count:16
Rebound 4.00 - 50.0 %4.00 - 50.0 %Average value: 20.6 % Grade Count:4
Bulk Modulus 4.30 - 5.00 GPa624 - 725 ksiAverage value: 4.60 GPa Grade Count:3
Shear Strength 0.965 - 1.14 MPa140 - 165 psiAverage value: 1.03 MPa Grade Count:5
Izod Impact, Notched 0.160 - 7.47 J/cm0.300 - 14.0 ft-lb/inAverage value: 1.28 J/cm Grade Count:89
Coefficient of Friction 2.50 - 3.302.50 - 3.30Average value: 2.80 Grade Count:3
Coefficient of Friction, Static 4.10 - 15.84.10 - 15.8Average value: 10.1 Grade Count:3
Tear Strength Test 17.2 - 29.017.2 - 29.0Average value: 23.2 Grade Count:3
Tear Strength 4.30 - 550 kN/m24.5 - 3140 pliAverage value: 51.2 kN/m Grade Count:554
Peel Strength 0.657 - 6.49 kN/m3.75 - 37.0 pliAverage value: 3.89 kN/m Grade Count:11
Taber Abrasion, mg/1000 Cycles 0.000 - 4700.000 - 470Average value: 67.7 Grade Count:77
Compression Set 3.00 - 580 %3.00 - 580 %Average value: 39.5 % Grade Count:372
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 8.00e+12 - 2.00e+16 ohm-cm8.00e+12 - 2.00e+16 ohm-cmAverage value: 8.69e+15 ohm-cm Grade Count:11
Surface Resistance 2.80e+16 ohm2.80e+16 ohmAverage value: 2.80e+16 ohm Grade Count:4
Dielectric Constant 2.40 - 5.662.40 - 5.66Average value: 3.90 Grade Count:21
Dielectric Strength 10.2 - 22.4 kV/mm260 - 570 kV/inAverage value: 15.6 kV/mm Grade Count:21
Dissipation Factor 0.0100 - 0.09500.0100 - 0.0950Average value: 0.0416 Grade Count:18
 
Thermal PropertiesMetricEnglishComments
CTE, linear 95.0 - 153 µm/m-°C52.8 - 85.0 µin/in-°FAverage value: 121 µm/m-°C Grade Count:15
Thermal Conductivity 0.140 - 0.390 W/m-K0.972 - 2.71 BTU-in/hr-ft²-°FAverage value: 0.284 W/m-K Grade Count:5
Melting Point 80.0 °C176 °FAverage value: 80.0 °C Grade Count:5
Maximum Service Temperature, Air 50.0 - 150 °C122 - 302 °FAverage value: 93.8 °C Grade Count:65
Deflection Temperature at 0.46 MPa (66 psi) 49.0 - 140 °C120 - 284 °FAverage value: 74.0 °C Grade Count:25
Working Point 40.0 - 45.0 °C104 - 113 °FAverage value: 42.5 °C Grade Count:5
Heat Distortion Temperature 45.0 - 129 °C113 - 264 °FAverage value: 65.7 °C Grade Count:23
Minimum Service Temperature, Air -60.0 - -3.40 °C-76.0 - 25.9 °FAverage value: -37.7 °C Grade Count:76
Brittleness Temperature -90.0 - -27.0 °C-130 - -16.6 °FAverage value: -62.3 °C Grade Count:33
Glass Transition Temp, Tg -46.0 - -40.0 °C-50.8 - -40.0 °FAverage value: -43.0 °C Grade Count:3
Flammability, UL94 HB - V-0HB - V-0Grade Count:24
Flash Point 18.9 - 213 °C66.0 - 415 °FAverage value: 168 °C Grade Count:19
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.50 - 1.501.50 - 1.50Average value: 1.50 Grade Count:4
Transmission, Visible 90.0 %90.0 %Average value: 90.0 % Grade Count:12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 4.44 - 175 °C40.0 - 347 °FAverage value: 62.3 °C Grade Count:24
Mold Temperature 20.0 - 82.2 °C68.0 - 180 °FAverage value: 48.7 °C Grade Count:20
Cure Time 0.0833 - 14400 min0.00139 - 240 hourAverage value: 1350 min Grade Count:181
 1.60 - 8640 min
@Temperature -10.0 - 204 °C
0.0267 - 144 hour
@Temperature 14.0 - 400 °F
Average value: 84.3 min Grade Count:425
Tack-Free Time 60.0 - 600 min1.00 - 10.0 hourAverage value: 255 min Grade Count:13
Pot Life 0.0330 - 270 min0.0330 - 270 minAverage value: 20.2 min Grade Count:87

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
Overview of materials for Thermoset Polyurethane, Elastomer, Glass Filled
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade
Overview of materials for Silicone Rubber

O5025 / 78458

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.