MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Bayhydrol® 110 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol 110 is an anionic dispersion of an aliphatic polyester urethane resin in water/n-methyl-2- pyrrolidone

Properties / Applications: Bayhydrol 110 polyurethane dispersion can be used in the formulation of ambient-cure or bake coatings for a wide range of rigid and flexible substrates such as wood, metal, vinyl-coated fabric, business machine housings and other plastic parts. This product has been developed to exhibit a combination of film hardness, flexibility, good water and abrasion resistance, and excellent solvent resistance. As with any product, use of Bayhydrol 110 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.07 g/cc
Volatiles 63 - 67 %g/ 120 min/ 110°C
pH 7.5 - 9.5
Viscosity 50 - 300 cP
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.7 MPa
Elongation at Break 180 %
100% Modulus 29.0 MPa
@Strain 100 %
Taber Abrasion, mg/1000 Cycles 12
@Load 1.00 kg
CS-17 wheel
 
Processing PropertiesOriginal ValueComments
Moisture Content 50 %
 
Descriptive Properties
AppearanceMilky white to brown liquid
Content15%n-methyl-2-pyrrolidone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Covestro Bayhydrol® A 242 Polyurethane Coating
Covestro Bayhydrol® A 2227/1 Polyurethane Coating
Covestro Bayhydrol® A 2058 Polyurethane Coating
Covestro Bayhydrol® A 145 Polyurethane Coating

PCOVEST0144 / 201927

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.