MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydrol® A 2058 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol A 2058 is an aqueous hydroxyfunctional polyacrylic dispersion. In the formulation of flexible two-component polyurethane top coats and primers for plastics.

Properties / Applications: Bayhydrol A 2058 is a hydrolysis-resistant polyacrylic dispersion neutralised with dimethyl ethanol amine. The product can be thinned with water to application viscosity. Bayhydrol A 2058 combined with Bayhydur 302 yields high-gloss flexible top coats which are resistant to solvents. The formulation can be applied as a one-coat system on many substrates and has good adhesion and body. Water-borne base coats formulated with, e.g. Bayhydrol UH 2952/1, can be overcoated with clear coats based on Bayhydrol A 2058. Two-pack primers can be formulated by combining Bayhydrol A 2058 with Bayhydur 302. These are highly suitable for use on thermoplastics and thermosets and are characterised by excellent adhesion, sandability and water resistance. Bayhydrol A 2058 has good pigment wetting properties and high shear stability. Sand and bead mills have proved suitable as grinding equipment. Pigments and extenders are added to a small amount of the total Bayhydrol content in the formulation. Deionised water is added to adjust the mixture to dispersion viscosity. Because of the good shear stability of the product, dispersion temperatures of up to 40°C have no negative effect. Depending on the co-reactants used, coatings formulated with Bayhydrol A 2058 can be dried for 45 min at 80°C. The pot life of systems applied under standard conditions (23°C, 60 ± 5% relative humidity) is approximately 1 hour. As with any product, use of Bayhydrol A 2058 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/cc
Volatiles 55 - 59 %55 - 59 %1g/1h/125 °C/convection oven
pH 7.5 - 9.57.5 - 9.51:3 in demineralized water
Viscosity 200 - 2000 cP200 - 2000 cPD=82s-1
 
Chemical PropertiesMetricEnglishComments
Acid Value 2525[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 100 °C>= 212 °F
 
Descriptive Properties
Content4.8%Hydroxyl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Covestro Bayhydrol® A 242 Polyurethane Coating
Covestro Bayhydrol® A 2227/1 Polyurethane Coating
Covestro Bayhydrol® A 145 Polyurethane Coating
Covestro Bayhydrol® 140 AQ Polyurethane Coating

PCOVEST0149 / 201932

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.