MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Bayhydrol® A 2227/1 Polyurethane Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings; Thermoset; Polyurethane, TS

Material Notes: Bayhydrol A 2227/1 is a polyester-polyacrylate dispersion. In the formulation of stoving industrial coatings with high whiteness retention on exposure to high temperatures. Also in the formulation of two-component polyurethane primers and top coats for plastics.

Properties / Applications: The viscosity of the product is highly dependent on the pH. As the pH may decrease during storage, a decrease in viscosity must also be expected. The viscosity can be restored to its original value by adding small amounts of an aqueous 10% solution of dimethyl ethanol amine. Stoving industrial coatings: To ensure optimum pigment wetting, the pH should be adjusted with aqueous dimethyl ethanol amine (10%) to between 8.5 and 9. Details can be found in the relevant guide formulations. Combined with melamine resins, Bayhydrol A 2227/1 can be used to formulate stoving top coats with less than 5% co-solvent content at application viscosity. The coatings cure at stoving conditions from 30 minutes at 120°C. The ratio of Bayhydrol A 2227/1 to amino resin (solids on solids) is usually 80 : 20. Given the many different amino resins available on the market, compatibility tests should always be carried out. As it is a hydroxyfunctional binder, Bayhydrol A 2227/1 is also suitable for use as a co-reactant for aqueous aliphatic polyisocyanates. An OH/NCO ratio of 1 : 1 should be used. To achieve good storage stabilities of coatings based on Bayhydrol A 2227/1 the pH of the coating should be adjusted to between 8.5 and 9 after formulation. Coatings for plastics: In the case of coatings for plastics, we recommend the use of Bayhydur 302. An OH/NCO ratio of 1 : 1.5 should be used. Bayhydrol A 2227/1 is characterized by its good pigment wetting properties and high shear stability. Bead and sand mills have proved suitable as grinding equipment. Grinding temperatures of up to approximately 50°C have no detrimental effect on quality of the coating. Given the many different pigments available, the storage stability should always be tested. The rutile titanium dioxide pigments of the Tronox range, especially Tronox® R-KB-4, are particularly suitable. As with any product, use of Bayhydrol A 2227/1 in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/cc
Volatiles 57 - 59 %57 - 59 %1g/1h/125 °C/convection oven
Particle Size <= 150 µm<= 150 µmMean
pH 7.5 - 8.57.5 - 8.51:3 in demineralized water
Viscosity 700 - 2500 cP700 - 2500 cPD= approx. 40 s-1
 
Chemical PropertiesMetricEnglishComments
Acid Value 7.0 - 107.0 - 10[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 98.0 °C>= 208 °F
 
Descriptive Properties
Content3.8%Hydroxyl
Minimum Film Forming Temperature<0°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lord Adhesives Chemglaze® V004 Polyurethane Coating
Covestro Bayhydrol® A 242 Polyurethane Coating
Covestro Bayhydrol® A 2058 Polyurethane Coating
Covestro Bayhydrol® A 145 Polyurethane Coating
Covestro Bayhydrol® 140 AQ Polyurethane Coating

PCOVEST0150 / 201933

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.