MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Saint-Gobain Fluran® F-5500-A Fluoroelastomer Tubing
Categories: Polymer

Material Notes: Fluran® Severe Environment Tubing has the physical and chemical characteristics that make it ideal for severe environments, such as dry cleaning fluid lines and solvent recovery systems, where other flexible tubings fail. It can be used in continuous service with temperatures as high as 400°F (204°C) and has excellent resistance to corrosive chemicals, oils, fuels, solvents and most mineral acids.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 g/cc1.90 g/ccASTM D792
Water Absorption 0.23 %0.23 %24 hrs; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 606015 sec.; ASTM D2240-02
Tensile Strength, Ultimate 9.65 MPa1400 psiASTM D412-98
Elongation at Break 300 %300 %ASTM D412-98
100% Modulus 2.41 MPa
@Strain 100 %
350 psi
@Strain 100 %
ASTM D412-98
Tear Strength 17.5 kN/m99.9 pliASTM D1004-94
Compression Set 37 %
@Temperature 70.0 °C
37 %
@Temperature 158 °F
22 hrs.; ASTM D395-02 Method B
Tensile Set 13 %13 %ASTM D412-98
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 19.7 kV/mm500 kV/inASTM D149-97
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Brittleness Temperature -51.0 °C-59.8 °FASTM D746-98
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
TIMCAL ENSACO™ 250G Conductive Carbon Black Compounds
Saint-Gobain Norton® OmniFlex™ Fluoroelastomer High Performance Seal Material (Milky White)
Mid-Mountain Materials ARMATEX® SF7 Silicone Rubber Coated Glass Fabric
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer
Chemours Viton® Z-200 Process Aid

PSTGQZ516 / 98147

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.