MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: A hard, colorable, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to create multilayer constructions offering bonding to textiles, metals, fluoroelastomers and PAs. In addition, it complies with FDA regulations for rubber articles intended for repeated use. This grade of Santoprene TPV is shear-dependent and can be processed on conventional thermoplastics equipment for extrusion. It is polyolefin based and completely recyclable.

Key Features:

  • EU and China RoHS compliant.
Applications:
  • Automotive – Weather Seals
  • Consumer Applications
Uses:
  • Automotive Applications
  • Hose
  • Metal Bonding
  • Profiles
  • Tie-Layers
Processing Method: Coextrusion, Extrusion and Profile Extrusion

Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South America

Information provided by ExxonMobil Chemical

Key Words: EU 2003/11/EC; RoHS Compliant, FDA 21 CFR 177.2600
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 86862 mm, 15 sec; ISO 868
Tensile Strength at Break 9.20 MPa1330 psiAcross Flow; ASTM D412
Tensile Stress at Strain 4.00 MPa
@Strain 100 %
580 psi
@Strain 100 %
Across Flow; ASTM D412
Elongation at Break 830 %830 %Across Flow; ASTM D412
 
Processing PropertiesMetricEnglishComments
Processing Temperature 185 - 260 °C365 - 500 °F
Adapter Temperature 216 - 232 °C421 - 450 °F
Die Temperature 216 - 232 °C421 - 450 °F
 
Compliance PropertiesMetricEnglishComments
FDA YesYes
 
Descriptive Properties
Change in Mass in IRM 903 Oil at 257°F for 70 hr37
ColorNatural Color
FormPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 273-40 Thermoplastic Elastomer
ExxonMobil Santoprene® 171-73 Thermoplastic Elastomer
ExxonMobil Santoprene® 251-85W232 Thermoplastic Elastomer
ExxonMobil Santoprene® 271-80 Thermoplastic Elastomer
ExxonMobil Santoprene® 8291-70PA Thermoplastic Elastomer

PADVA144 / 22834

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.