MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemours Viton® Z-200 Process Aid
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer

Material Notes: Description: Viton® FreeFlow™ Z200 is a process aid for polyolefins combining an improved rheology fluoroelastomer with a highly thermally stable surface active agent to provide outstanding process aid performance through the full range of polyolefin processing conditions. Viton® FreeFlow™ Z200 eliminates melt fracture, reduces die pressure and torque, reduces power requirements and reduces die buildup. Viton® FreeFlow™ Z200 incorporates a highly efficient surface active agent which gives excellent process aid performance even under the most severe line conditions. It conditions quickly and efficiently and can tolerate higher processing temperatures than other fluoroelastomer processing aids.

Advantages:

  • Improved rates of conditioning when starting new lines or purged systems
  • Improved performance on difficult to condition lines or with difficult formulations without the need for high additive levels often required with current process aids
  • Improved economics
  • Excellent thermal stability (up to 300°C) for cast film lines where other additives show degradation
  • Improved performance in combined masterbatches with pigments
  • Improved resistance to interactions
  • Applications for food contact approval have been filled

Information provided by manufacturer.

Chemours was formed from former DuPont performance chemicals businesses, including the Viton product line, in 2015.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.15 - 1.25 g/cc0.0415 - 0.0452 lb/in³
 
Descriptive Properties
AppearanceWhite, free-flowing powder
Package Stability5 yr
Packaging20 kg bag in box or 60 kg fiber drum

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chemours Viton® GFLT-600S with ZnO Fluoroelastomer Compound
Chemours Viton® GF-600S with 3phr, DBPH50-HP Fluoroelastomer Compound
Mid-Mountain Materials ARMATEX® SF7 Silicone Rubber Coated Glass Fabric
ExxonMobil Santoprene® 8291-85TL Thermoplastic Elastomer
Chemours Viton® GF-600S with 3phr, DCP-40KE Fluoroelastomer Compound

PDVDA64 / 34033

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.