MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Refractory Metals

(Viewing data as-entered. Click here to return)
Molybdenum, Mo, Stress Relieved
Categories: Metal; Nonferrous Metal; Molybdenum Alloy; Pure Element

Material Notes: Physical Form: Gray-Black Metal; Cubic. Stress relieved applies only to tensile values; other property values are typical of the element.

Key Words: Moly
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Elmet Technologies is a 100% US owned and operated, fully integrated manufacturer of Molybdenum, Tungsten and related alloys such as TZM, WHA & MoLa. At our 220,000 sqr/ft plant in Lewiston, Maine, Elmet manufactures W & Mo pure powders plus rod, wire, plate, sheet & foil in additional to offering fabrication and machining services. ITAR, ISO and AS9100 registered. www.elmettechnologies.com

PLANSEE SE: Whether it's high temperatures, aggressive chemicals or extreme mechanical loading: PLANSEE supplies a suitable product solution in refractory metals or composite materials. As the world market leader in powder metallurgically produced high performance materials we combine outstanding materials knowledge with profound applications and technology know-how. Visit us at www.plansee.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 10.22 g/cc
a Lattice Constant 3.147 Å
@Temperature 25.0 °C
Body Centered Cubic
Vapor Pressure 1.00 torr
@Temperature 3102 °C
 10.0 torr
@Temperature 3555 °C
 100 torr
@Temperature 4109 °C
 200 torr
@Temperature 4322 °C
 400 torr
@Temperature 4553 °C
 760 torr
@Temperature 4804 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 95.94
Atomic Number 42
Atomic Volume 1.53e-029m^3
Thermal Neutron Cross Section 2.5 barns/atom
X-ray Absorption Edge 0.61977 ÅK
 4.32066 ÅLI
 4.7133 ÅLII
 4.9093 ÅLIII
Electrode Potential -0.200 V
Electronegativity 2.16Pauling
Ionic Radius 0.620 ÅCrystal Ionic Radius for Valence +6
 0.700 ÅCrystal Ionic Radius for Valence +4
 0.930 ÅCrystal Ionic Radius for Valence +1
Electrochemical Equivalent 1.79 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 52.0 ksi
@Temperature 982 °C
Stress Relief Annealed
Tensile Strength, Ultimate 515 MPa
Tensile Strength, Yield 415 MPa
@Strain 0.2 %
Elongation at Break 2.0 - 17 %in 50 mm
Rupture Strength 25000 psi
@Temperature 982 °C,
Time 36000 sec
Stress Relief Annealed
Modulus of Elasticity 330 GPa
 160 GPa
@Temperature 2000 °C
 200 GPa
@Temperature 1800 °C
 250 GPa
@Temperature 1400 °C
 275 GPa
@Temperature 1000 °C
Compressive Yield Strength 400 MPa0.01% Yield
Bulk Modulus 272 GPa
Poissons Ratio 0.38calculated
Shear Modulus 120 GPa
Shear Strength 500 MPatorsional strain rate 0.25/sec
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000570 ohm-cm
 0.00000520 ohm-cm
@Temperature 0.000 °C
 0.00000570 ohm-cm
@Temperature 27.0 °C
 0.0000239 ohm-cm
@Temperature 727 °C
 0.0000292 ohm-cm
@Temperature 927 °C
 0.0000352 ohm-cm
@Temperature 1127 °C
 0.0000412 ohm-cm
@Temperature 1327 °C
 0.0000472 ohm-cm
@Temperature 1527 °C
 0.0000535 ohm-cm
@Temperature 1727 °C
 0.0000595 ohm-cm
@Temperature 1927 °C
 0.0000660 ohm-cm
@Temperature 2127 °C
 0.0000692 ohm-cm
@Temperature 2227 °C
 0.0000718 ohm-cm
@Temperature 2327 °C
 0.0000782 ohm-cm
@Temperature 2527 °C
 0.0000814 ohm-cm
@Temperature 2622 °C
Magnetic Susceptibility 9.3e-7cgs/g
Critical Magnetic Field Strength, Oersted 93 - 99
Critical Superconducting Temperature 0.910 - 0.920 K
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 293 J/g
Heat of Vaporization 5610 J/g
CTE, linear 5.35 µm/m-°C
@Temperature 20.0 °C
 6.00 µm/m-°C
@Temperature 0.000 - 250 °C
 6.00 µm/m-°C
@Temperature 0.000 - 500 °C
 6.50 µm/m-°C
@Temperature 0.000 - 1000 °C
Specific Heat Capacity 0.217 J/g-°CGas
 0.255 J/g-°C
Thermal Conductivity 138 W/m-K
 100 W/m-K
@Temperature 1127 °C
 105 W/m-K
@Temperature 927 °C
 112 W/m-K
@Temperature 727 °C
 118 W/m-K
@Temperature 527 °C
 126 W/m-K
@Temperature 327 °C
 130 W/m-K
@Temperature 227 °C
 134 W/m-K
@Temperature 127 °C
 138 W/m-K
@Temperature 27.0 °C
 143 W/m-K
@Temperature -73.0 °C
 150 W/m-K
@Temperature -263 °C
 179 W/m-K
@Temperature -173 °C
 210 W/m-K
@Temperature -193 °C
 250 W/m-K
@Temperature -213 °C
 280 W/m-K
@Temperature -253 °C
 350 W/m-K
@Temperature -233 °C
Melting Point 2617 °C
Boiling Point 4639 °C
Heat of Formation 0.000 kJ/molCrystal
 658.1 kJ/molGas
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.17
@Temperature 100 °C
total spectrum
Reflection Coefficient, Visible (0-1) 0.46500 nm
 
Component Elements PropertiesOriginal ValueComments
Molybdenum, Mo 100 %
 
Descriptive Properties
CAS Number7439-98-7
SolubilityInsoluble in H2O, diluted Acid and Alkaline

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Molybdenum, Mo, Annealed
Molybdenum, Mo, Recrystallized
Tungsten, W
Nickel, Ni
Manganese, Mn

AMEMo01 / 62

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.