MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Manganese, Mn
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: Hard Gray Metal. It is almost never used unalloyed, but it is a very important alloying component in a wide variety of steel and other alloys.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.44 g/cc0.269 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 54.9380554.9380554.938049 - 1995
Atomic Number 2525
Thermal Neutron Cross Section 12.6 barns/atom12.6 barns/atom
X-ray Absorption Edge 1.896 Å1.896 ÅK
 16.268 Å16.268 ÅLI
 18.896 Å18.896 ÅLII
 19.2484 Å19.2484 ÅLIII
Electrode Potential -1.05 V-1.05 V
Electronegativity 1.551.55Pauling
Ionic Radius 0.460 Å0.460 ÅCrystal Ionic Radius for Valence +7
 0.600 Å0.600 ÅCrystal Ionic Radius for Valence +4
 0.660 Å0.660 ÅCrystal Ionic Radius for Valence +3
 0.800 Å0.800 ÅCrystal Ionic Radius for Valence +2
Electrochemical Equivalent 0.684 g/A/h0.684 g/A/htrivalent
 1.025 g/A/h1.025 g/A/hdivalent
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 460460Converted from Vickers for 3000 kg load/10 mm ball Brinell test.
Hardness, Rockwell A 7575Converted from Vickers.
Hardness, Rockwell C 4848Converted from Vickers.
Hardness, Vickers 500500
Tensile Strength, Ultimate 496 MPa71900 psiGamma Phase
Tensile Strength, Yield 241 MPa35000 psiGamma Phase
Modulus of Elasticity 159 GPa23100 ksi
Bulk Modulus 92.6 GPa13400 ksi
Poissons Ratio 0.350.35
Shear Modulus 76.4 GPa11100 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00000688 ohm-cm
@Temperature -273 °C
0.00000688 ohm-cm
@Temperature -459 °F
 0.00001884 ohm-cm
@Temperature -263 °C
0.00001884 ohm-cm
@Temperature -441 °F
 0.0000536 ohm-cm
@Temperature -253 °C
0.0000536 ohm-cm
@Temperature -423 °F
 0.0001261 ohm-cm
@Temperature -223 °C
0.0001261 ohm-cm
@Temperature -369 °F
 0.0001321 ohm-cm
@Temperature -173 °C
0.0001321 ohm-cm
@Temperature -279 °F
 0.0001359 ohm-cm
@Temperature -123 °C
0.0001359 ohm-cm
@Temperature -189 °F
 0.0001391 ohm-cm
@Temperature -73.0 °C
0.0001391 ohm-cm
@Temperature -99.4 °F
 0.0001419 ohm-cm
@Temperature -23.0 °C
0.0001419 ohm-cm
@Temperature -9.40 °F
 0.000143 ohm-cm
@Temperature 0.000 °C
0.000143 ohm-cm
@Temperature 32.0 °F
 0.000144 ohm-cm
@Temperature 20.0 °C
0.000144 ohm-cm
@Temperature 68.0 °F
 0.0001442 ohm-cm
@Temperature 27.0 °C
0.0001442 ohm-cm
@Temperature 80.6 °F
 0.0001461 ohm-cm
@Temperature 77.0 °C
0.0001461 ohm-cm
@Temperature 171 °F
 0.0001477 ohm-cm
@Temperature 127 °C
0.0001477 ohm-cm
@Temperature 261 °F
 0.0001501 ohm-cm
@Temperature 227 °C
0.0001501 ohm-cm
@Temperature 441 °F
 0.0001521 ohm-cm
@Temperature 327 °C
0.0001521 ohm-cm
@Temperature 621 °F
 0.0001536 ohm-cm
@Temperature 427 °C
0.0001536 ohm-cm
@Temperature 801 °F
Magnetic Susceptibility 0.00001150.0000115cgs/g
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 271 J/g117 BTU/lb
Heat of Vaporization 4091 J/g1760 BTU/lb
CTE, linear  22.8 µm/m-°C
@Temperature 20.0 - 100 °C
12.7 µin/in-°F
@Temperature 68.0 - 212 °F
 26.9 µm/m-°C
@Temperature 227 °C
14.9 µin/in-°F
@Temperature 441 °F
 45.7 µm/m-°C
@Temperature 1087 °C
25.4 µin/in-°F
@Temperature 1989 °F
Beta Phase
Specific Heat Capacity 0.379 J/g-°C0.0906 BTU/lb-°FGas
 0.448 J/g-°C0.107 BTU/lb-°F
Thermal Conductivity  1.64 W/m-K
@Temperature -263 °C
11.4 BTU-in/hr-ft²-°F
@Temperature -441 °F
 2.42 W/m-K
@Temperature -253 °C
16.8 BTU-in/hr-ft²-°F
@Temperature -423 °F
 4.07 W/m-K
@Temperature -223 °C
28.2 BTU-in/hr-ft²-°F
@Temperature -369 °F
 5.81 W/m-K
@Temperature -173 °C
40.3 BTU-in/hr-ft²-°F
@Temperature -279 °F
 6.65 W/m-K
@Temperature -123 °C
46.2 BTU-in/hr-ft²-°F
@Temperature -189 °F
 7.18 W/m-K
@Temperature -73.0 °C
49.8 BTU-in/hr-ft²-°F
@Temperature -99.4 °F
 7.54 W/m-K
@Temperature -23.0 °C
52.3 BTU-in/hr-ft²-°F
@Temperature -9.40 °F
 7.68 W/m-K
@Temperature 0.000 °C
53.3 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
 7.79 W/m-K
@Temperature 20.0 °C
54.1 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 7.82 W/m-K
@Temperature 27.0 °C
54.3 BTU-in/hr-ft²-°F
@Temperature 80.6 °F
Melting Point 1244 °C2271 °F
Boiling Point 2061 °C3742 °F
Heat of Formation 0.000 kJ/mol0.000 kJ/molCrystal
 280.7 kJ/mol280.7 kJ/molGas
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.570.57unoxidized, 650 nm, total spectrum
Reflection Coefficient, Visible (0-1) 0.450.45400 nm air-exposed
 0.550.55400 nm polished
 
Component Elements PropertiesMetricEnglishComments
Manganese, Mn 100 %100 %
 
Descriptive Properties
CAS Number7439-96-5
SolubilitySoluble in diluted Acids

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper, Cu; Annealed
Iron, Fe
Silver, Ag
Nickel, Ni
Chromium, Cr; Recrystallized

AMEMn00 / 60

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.