MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Aremco-Bond™ 598 Conductive Epoxy Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: Electrically and thermally conductive, nickel-filled, single part system. Low viscosity, inorganic coating for applications to 1000 ºF (540 °C).

Key Words: Coatings
Vendors: Aremco offers a broad line of electrically and thermally conductive adhesives and greases for applications from room temperature to 1700°F (927°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.90 g/cc
 
Mechanical PropertiesOriginal ValueComments
Adhesive Bond Strength 9.48 MPaPer ASTM D1002-94; shear strength of single lap-joint metal coupons in tension loading.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1e+05
Dielectric Strength 9.80 kV/mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 33.7 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 1.20 W/m-K
Maximum Service Temperature, Air 1000 °F
 
Processing PropertiesOriginal ValueComments
Pot Life 240 min

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco Aremco-Seal™ 4030 High Temperature Specialty Coatings Silicone, Ceramic Filled
Aremco Aremco-Bond™ 860 Thermally Conductive Material, Aluminum Nitride Filled
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Raschig Group EPOXIDUR® 3585 EP Epoxy, Molded, Glass Fiber Filler
Lord Adhesives Thermoset™ ME-542 Underfill Encapsulant

ZPAR075 / 24247

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.