MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, High Temperature

Material Notes: Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing.

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Aremco

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
Linear Mold Shrinkage 0.0031 cm/cm0.0031 in/incure shrinkage
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090
Flexural Strength 93.8 MPa13600 psi
Shear Strength 13.8 MPa2000 psi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+15 ohm-cm2.00e+15 ohm-cm
Dielectric Constant 4.8
@Frequency 1000 Hz
4.8
@Frequency 1000 Hz
Dielectric Strength 17.7 kV/mm450 kV/in
Dissipation Factor 0.000700.00070
 
Thermal PropertiesMetricEnglishComments
CTE, linear 25.2 µm/m-°C14.0 µin/in-°F
Maximum Service Temperature, Air 300 °C572 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
Step 1 of recommended 2 step cure
 120 min
@Temperature 177 °C
2.00 hour
@Temperature 350 °F
Step 2 of recommended 2 step cure
 480 min
@Temperature 149 °C
8.00 hour
@Temperature 300 °F
Alternate
Pot Life 90.0 min
@Temperature 25.0 °C
90.0 min
@Temperature 77.0 °F
100 g mass
 
Descriptive Properties
Chemical ResistanceExcellent
ColorBeige
Mix Ratio by weight100:5.5resin:hardener
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BCC Products BC 6004 Epoxy Surface Coat
Trelleborg Emerson & Cuming Stycast® 2762/17M-1 Two-Component Epoxy High Service Temp Encapsulant
Master Bond EP17 One Component Epoxy, Heat Curing Structural Adhesive/Sealant
Trelleborg Emerson & Cuming Stycast® 4952/25 Two-Component Silicone High Service Temp Encapsulant
Trelleborg Emerson & Cuming Stycast® W-66/17M-1 Two-Component Epoxy High Service Temp Encapsulant

PAREM96e / 178190

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.