MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

Master Bond EP17 One Component Epoxy, Heat Curing Structural Adhesive/Sealant
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy, High Temperature

Material Notes: Product Description: Master Bond Polymer System EP17 is a toughened one component heat curing epoxy resin system featuring high shear strength and very high temperature resistance. This one component system is formulated to cure at 300°F for 90-120 minutes or at 350°F for 60-90 minutes. EP17 has a tensile shear strength in excess of 3,500 psi. The service temperature range extends from -100°F up to 600°F. EP17 forms toughened and dimensionally stable bonds with minimal shrinkage upon cure. It is 100% reactive and does not contain any solvents or diluents. EP17 has a paste consistency. EP17 possesses high physical strength properties and is readily machinable. As a one part system EP17 is easy to handle. It does not require mixing prior to use and has an unlimited working life at room temperature. It bonds well to a wide variety of substrates including metals, glass, ceramics, vulcanized rubbers and many plastics. It has excellent resistance to a wide range of chemicals including fuels, acids, bases, oils and many solvents. The standard color is tan. EP17 is an excellent electrical insulator.

Product Advantages:

  • Single component system; no mixing prior to use. Long working life at room temperature.
  • Easy application; contact pressure only required during heat cure.
  • High tensile shear and compressive strength.
  • 100% reactive. Contains no solvents or volatiles.
  • Exceptional high temperature resistance. Serviceable up to 600°F.
  • Bonds well to a wide range of substrates.
  • Good electrical insulation properties and outstanding chemical resistance.
  • Superior dimensional stability.
  • Very low shrinkage upon cure.
  • Excellent toughness

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 80>= 80
Tensile Strength 58.6 MPa8500 psi
Elongation at Break 3.4 %3.4 %
Tensile Modulus 2.41 GPa350 ksi
Compressive Strength 207 MPa30000 psi
Adhesive Bond Strength 23.8 MPa3450 psiafter 30 days water immersion
 24.1 MPa3500 psiTensile lap, Aluminum to Aluminum
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  >= 1.00e+13 ohm-cm
@Temperature 149 °C
>= 1.00e+13 ohm-cm
@Temperature 300 °F
 >= 1.00e+15 ohm-cm
@Temperature 23.9 °C
>= 1.00e+15 ohm-cm
@Temperature 75.0 °F
Dielectric Constant  4.5
@Frequency 60 Hz,
Temperature 23.9 °C
4.5
@Frequency 60 Hz,
Temperature 75.0 °F
 4.6
@Frequency 60 Hz,
Temperature 149 °C
4.6
@Frequency 60 Hz,
Temperature 300 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 288 °C550 °F
Minimum Service Temperature, Air -101 °C-150 °F
Glass Transition Temp, Tg 178 °C352 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  60.0 - 90.0 min
@Temperature 177 °C
1.00 - 1.50 hour
@Temperature 350 °F
 90.0 - 120 min
@Temperature 149 °C
1.50 - 2.00 hour
@Temperature 300 °F
Shelf Life 8.00 Month
@Temperature 4.44 - 10.0 °C
8.00 Month
@Temperature 40.0 - 50.0 °F
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound
Abatron AboCast/AboCure 8501-4/8501-4 High Temperature Resistant Epoxy
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy

PMASTM808 / 185401

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.