MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Bond™ 860 Thermally Conductive Material, Aluminum Nitride Filled
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Thermally Conductive, Aluminum Nitride Filled, 1:1 Epoxy Paste.
Exceptional Mechanical and Thermal Properties to 400 ºF.

Vendors: Aremco’s High Performance Epoxies provide a wide range of solutions for bonding ceramics, composites, glass, metals, plastics, and other materials. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.90 g/cc1.90 g/cc
Particle Size <= 10 µm<= 10 µm
Viscosity 40000 cP40000 cPmixed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7575
Shear Strength 9.480 MPa1375 psiStrength can be increased 40-50% by heat curing; ASTM D1002-94
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 34.2 µm/m-°C
@Temperature 20.0 °C
19.0 µin/in-°F
@Temperature 68.0 °F
Thermal Conductivity 1.22 W/m-K8.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C400 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  120 min
@Temperature 93.3 °C
2.00 hour
@Temperature 200 °F
Recommended Cure
 1440 - 2880 min
@Temperature 23.0 °C
24.0 - 48.0 hour
@Temperature 73.4 °F
Alternate Cure
Pot Life 240 min
@Temperature 25.0 °C
240 min
@Temperature 77.0 °F
100 gm mass
 
Descriptive Properties
Chemical ResistanceExcellent
ColorGray
Mix Ratio by Weight1:1resin:hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramacast™ 675 High Temperature Potting & Casting Material Aluminum Nitride
Acerde Aluminum Nitride
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled
Sapco Aluminum Nitride
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride

PAREM25 / 24289

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.