Hostacom TRC787Y NATURAL is a thermoplastic polyolefin elastomeric compound for injection molding. It is typically used for fully painted automotive interior parts including instrument panels, doors, and consoles. It has an excellent balance of processability, rigidity, and excellent impact strength. Applications: Instrument Panels, Interior Automotive ApplicationsInformation provided by LyondellBasell. |