MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: MAGNUM™ 3325SLG is a medium heat ABS. It is very gloss combined with a high flow makes it specifically suitable for unpainted interior automotive applications. MAGNUM™ 3325SLG can thereby help save up to 50% of the part costs.

Benefits:

  • Self-coloring enabling improvement of costs by using less pigments and lowering your logistic costs
  • Low VOC allowing a better interior air quality facing increasing regulatory and OEMs constraints
  • Heat stability during wide range of processing temperatures: enhanced part design freedom
  • High scratch and mar resistance for an improved aesthetic durability of the parts
  • Easier recyclability of unpainted part
Applications:
  • Matte/unpainted interior automotive applications
  • Mid-consoles
  • Pillars
  • Door liners
  • Glove boxes
Automotive Specifications:
  • CHRYSLER MS-DB-191 Type A
  • FORD WSS-M4D827-C1
  • GM GMW 15572P-ABS-T2
  • FORD WSS-M4D827-A
  • GM GMP.ABS.003

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³ASTM D792
Apparent Bulk Density 0.690 g/cc0.0249 lb/in³ASTM D1895
Linear Mold Shrinkage, Flow 0.0053 cm/cm0.0053 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0052 cm/cm0.0052 in/inISO 294-4
Melt Flow 3.1 g/10 min
@Load 3.80 kg,
Temperature 230 °C
3.1 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 37.0 MPa5370 psiISO 527-2/50
 40.0 MPa5800 psi51 mm/min; ASTM D638
Elongation at Break 19 %19 %ISO 527-2/50
 22 %22 %51 mm/min; ASTM D638
Elongation at Yield 2.8 %2.8 %51 mm/min; ASTM D638
 2.8 %2.8 %ISO 527-2/50
Tensile Modulus 1.92 GPa278 ksiISO 527-2/50
 2.08 GPa302 ksi51 mm/min; ASTM D638
Flexural Strength 61.0 MPa8850 psi2.0 mm/min, 3-points; ISO 178
 64.1 MPa9300 psiMethod I (3 point load), 1.3 mm/min; ASTM D790
Flexural Modulus 2.07 GPa300 ksi2.0 mm/min, 3-points; ISO 178
 2.41 GPa350 ksiMethod I (3 point load), 1.3 mm/min; ASTM D790
Izod Impact, Notched  1.30 J/cm
@Temperature -30.0 °C
2.44 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 1.90 J/cm
@Temperature 23.0 °C
3.56 ft-lb/in
@Temperature 73.4 °F
ASTM D256
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 180/A
 18.0 kJ/m²
@Temperature 23.0 °C
8.57 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact, Notched  1.10 J/cm²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.60 J/cm²
@Temperature 23.0 °C
7.61 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Dart Drop, Total Energy  23.0 J
@Temperature -30.0 °C
17.0 ft-lb
@Temperature -22.0 °F
Peak; ASTM D3763
 30.0 J
@Temperature 23.0 °C
22.1 ft-lb
@Temperature 73.4 °F
Peak; ASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 83.0 µm/m-°C
@Temperature -40.0 - 110 °C
46.1 µin/in-°F
@Temperature -40.0 - 230 °F
ASTM E831
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature -40.0 - 110 °C
50.0 µin/in-°F
@Temperature -40.0 - 230 °F
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 96.7 °C206 °FUnannealed; ASTM D648
 97.0 °C207 °FUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C180 °FUnannealed; ASTM D648
Vicat Softening Point 101 °C214 °FASTM D1525
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 238 °C460 °F
Middle Barrel Temperature 249 °C480 °F
Front Barrel Temperature 254 °C489 °F
Nozzle Temperature 249 - 254 °C480 - 489 °F
Melt Temperature 243 - 271 °C469 - 520 °F
Mold Temperature 38.0 - 66.0 °C100 - 151 °F
Drying Temperature 82.0 - 85.0 °C180 - 185 °F
Dry Time >= 2.00 hour>= 2.00 hour

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI
LyondellBasell Hostacom TRC787N 600R JET BLK Thermoplastic Olefinic Elastomer
RTP Company RTP PP 20 GF NAT Polypropylene (PP); Value Product - Glass Fiber - Chemically Coupled
Covestro Bayblend® T50 XF Polycarbonate + ABS

PDWST075 / 142284

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.