MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

DuPont Mobility and Materials Zytel® ST801 BK010A PA66-HI  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Super Toughened Polyamide 66

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³DAM; ISO 1183
Melt Density 0.920 g/cc
@Temperature >=263 °C
0.0332 lb/in³
@Temperature >=505 °F
Water Absorption 6.5 %
@Thickness 2.00 mm
6.5 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Moisture Absorption 2.00 %
@Thickness 2.00 mm
2.00 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Number 156 cm³/g1.56 dl/gDAM; ISO 307, 1157, 1628
Linear Mold Shrinkage, Flow 0.018 cm/cm0.018 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 43.0 MPa6240 psi50% RH; ISO 527-1/-2
 50.0 MPa7250 psiDAM; ISO 527-1/-2
Film Elongation at Yield, MD 5.7 %5.7 %DAM; ISO 527-3
Elongation at Break 32 %32 %DAM; ISO 527-1/-2
 >= 50 %>= 50 %50% RH; ISO 527-1/-2
Elongation at Yield 5.7 %5.7 %DAM; ISO 527-1/-2
 37 %37 %50% RH; ISO 527-1/-2
Tensile Modulus 0.900 GPa131 ksi50% RH; ISO 527-1/-2
 2.00 GPa290 ksiDAM; ISO 527-1/-2
Poissons Ratio 0.400.40DAM; ISO 527-1/-2
 0.450.4550%RH; ISO 527-1/-2
Izod Impact, Unnotched (ISO)  80.0 kJ/m²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 90.0 kJ/m²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 1.80 J/cm²
@Temperature -30.0 °C
8.57 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 12.0 J/cm²
@Temperature 23.0 °C
57.1 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
Tensile Creep Modulus, 1 hour 800 MPa116000 psi50% RH; ISO 899-1
Tensile Creep Modulus, 1000 hours 700 MPa102000 psi50% RH; ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cm50% RH; IEC 62631-3-1
 1.00e+15 ohm-cm1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 1.00e+15 ohm1.00e+15 ohm50% RH; IEC 62631-3-2
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
DAM; IEC 62631-2-1
 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 8.0
@Frequency 100 Hz
8.0
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 31.0 kV/mm787 kV/inDAM; IEC 60243-1
Dissipation Factor  0.0080
@Frequency 100 Hz
0.0080
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.014
@Frequency 1e+6 Hz
0.014
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.055
@Frequency 1e+6 Hz
0.055
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 0.18
@Frequency 100 Hz
0.18
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 120 µm/m-°C66.7 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FDAM; ISO 11359-1/-2
Melting Point 263 °C505 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 150 °C302 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °C147 °FDAM; ISO 75-1/-2
Vicat Softening Point 205 °C401 °F50°C/h, 50N; ISO 306
Glass Transition Temp, Tg 75.0 °C167 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread 26.0 mm/min
@Thickness 1.00 mm
1.02 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
Oxygen Index 20 %20 %DAM; ISO 4589-1/-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection
 290 °C554 °FInjection Optimum
Mold Temperature 50.0 - 100 °C122 - 212 °FInjection
 80.0 °C176 °FInjection Optimum
Ejection Temperature 190 °C374 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourDehumidified Dryer; Injection
Moisture Content 0.20 %0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiInjection
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Drying RecommendedyesInjection
FMVSS ClassBISO 3795 (FMVSS 302)
Hold pressure time (s/mm)4Injection
Max. screw tangential speed (m/s)0.3Injection
Part Marking CodePA66-HIISO 11469
ProcessingInjection Molding
 Other Extrusion
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPA66-HIISO 1043
Special characteristicsLight stabilized or stable to light
 U.V. stabilized or stable to weather

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® ST801 NC010A PA66-HI
Trinseo MAGNUM™ 3325 MT Acrylonitrile Butadiene Styrene (ABS) Resin
LyondellBasell Hostacom TRC787N 600R JET BLK Thermoplastic Olefinic Elastomer
Clariant Renol PA101F/ST801 Nylon 66, Impact Modified, Lubricated
Celanese Zytel® 101 NC010 PA66

PDSX5508 / 198148

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.