MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Extreme Materials from MCAM
Visit Mitsubishi Chemical Advanced Materials for Extreme Materials - high performance plastic machining stock engineered to replace metals such as nickel alloys or stainless steel.

(Viewing data as-entered. Click here to return)
Sandvik Nikrothal 60 Resistance Wire
Categories: Metal; Nonferrous Metal; Nickel Alloy; Superalloy; Iron Base

Material Notes: NIKROTHAL 60 can be used at operating temperatures up to 1150°C (2100°F). NIKROTHAL 60 has excellent hot strength, good oxidation properties and very good formability. NIKROTHAL 60 has good corrosion resistance except in sulphur containing atmospheres and certain controlled atmospheres. NIKROTHAL 60 is used as electric heating element material in domestic appliances and furnace applications up to high temperatures.

Typical applications for NIKROTHAL 60 are in metal sheathed tubular elements used in hot plates, grills, toaster ovens, storage heaters, etc and as suspended coils in air heaters used in clothes dryers, fan heaters, hand dryers

Information provided by Sandvik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.20 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 160
@Thickness 4.00 mm
 180
@Thickness 1.00 mm
Tensile Strength, Ultimate 100 MPa
@Temperature 900 °C
deformation rate= 6.2x10-2/min
 700 MPa
@Thickness 4.00 mm
 730 MPa
@Thickness 1.00 mm
Tensile Strength, Yield 300 MPa
@Strain 0.2 %,
Thickness 4.00 mm
 370 MPa
@Strain 0.2 %,
Thickness 1.00 mm
Elongation at Break 30 %
@Thickness 4.00 mm
 35 %
@Thickness 1.00 mm
Creep Strength 4.00 MPa
@Temperature 1000 °C,
Time 3.60e+6 sec
1% elongation
 15.0 MPa
@Temperature 800 °C,
Time 3.60e+6 sec
1% elongation
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000111 ohm-cm
 0.000113 ohm-cm
@Temperature 100 °C
 0.000115 ohm-cm
@Temperature 200 °C
 0.000116 ohm-cm
@Temperature 300 °C
 0.000117 ohm-cm
@Temperature 400 °C
 0.000120 ohm-cm
@Temperature 500 °C
 0.000121 ohm-cm
@Temperature 600 °C
 0.000121 ohm-cm
@Temperature 700 °C
 0.000122 ohm-cm
@Temperature 800 °C
 0.000122 ohm-cm
@Temperature 900 °C
 0.000123 ohm-cm
@Temperature 1000 °C
 0.000124 ohm-cm
@Temperature 1100 °C
 0.000125 ohm-cm
@Temperature 1200 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.0 µm/m-°C
@Temperature 20.0 - 250 °C
 15.0 µm/m-°C
@Temperature 20.0 - 500 °C
 16.0 µm/m-°C
@Temperature 20.0 - 750 °C
 17.0 µm/m-°C
@Temperature 20.0 - 1000 °C
Specific Heat Capacity 0.460 J/g-°C
@Temperature 20.0 °C
 0.460 J/g-°C
@Temperature 100 °C
 0.480 J/g-°C
@Temperature 200 °C
 0.500 J/g-°C
@Temperature 300 °C
 0.530 J/g-°C
@Temperature 400 °C
 0.550 J/g-°C
@Temperature 500 °C
 0.580 J/g-°C
@Temperature 600 °C
 0.600 J/g-°C
@Temperature 700 °C
 0.630 J/g-°C
@Temperature 800 °C
 0.660 J/g-°C
@Temperature 900 °C
 0.670 J/g-°C
@Temperature 1000 °C
 0.710 J/g-°C
@Temperature 1100 °C
Thermal Conductivity 13.0 W/m-K
@Temperature 20.0 °C
 13.0 W/m-K
@Temperature 100 °C
 14.0 W/m-K
@Temperature 200 °C
 16.0 W/m-K
@Temperature 300 °C
 17.0 W/m-K
@Temperature 400 °C
 19.0 W/m-K
@Temperature 500 °C
 20.0 W/m-K
@Temperature 600 °C
 22.0 W/m-K
@Temperature 700 °C
 24.0 W/m-K
@Temperature 800 °C
 25.0 W/m-K
@Temperature 900 °C
 28.0 W/m-K
@Temperature 1000 °C
 29.0 W/m-K
@Temperature 1100 °C
Melting Point 1390 °C
Maximum Service Temperature, Air 1150 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.88fully oxidized
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.10 %
Chromium, Cr 14 - 18 %
Iron, Fe >= 19.2 %
Manganese, Mn <= 1.0 %
Nickel, Ni 57 - 60 %
Silicon, Si 1.0 - 1.7 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nichrome 60-15 Medium Temperature Resistor Material
Special Metals INCONEL® C276 Nickel Superalloy Plate
Sandvik Nikrothal 60 Resistance Strip
Sandvik Nikrothal 60 Resistance Ribbon
Hoskins Manufacturing Chromel® Thermocouple Wire

NSANDV076 / 18970

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.