MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
3M 9471 Adhesive Transfer Tapes with Adhesive 300
Categories: Polymer; Adhesive

Material Notes: 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive family is available in several thicknesses for a wide variety of surface bonding and provides a variety of liner configurations to help ensure excellent process flexibility.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 2.00 milAdhesive
 3.50 milLiner
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.00 pliPolypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
 2.25 pliPolypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
 3.1875 pliStainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
 3.1875 pliPolycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr RT; ASTM D3330
 4.6875 pliPolycarbonate, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
 5.3125 pliStainless Steel, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 3.21
@Frequency 1000 Hz
0.040 thickness; ASTM D-150-92
Dielectric Strength 340 kV/in
@Thickness 0.0508 mm
500 vac, rms. [60 Hz]/sec; ASTM D149-92
Dissipation Factor 0.040
@Thickness 0.0508 mm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 58.0 µm/m-°CSecond heat; ASTM-D696
 20.0 µm/m-°C
@Thickness 0.0508 mm
First heat; ASTM-D696
 
Processing PropertiesOriginal ValueComments
Shelf Life 18.0 Month
 
Descriptive Properties
Adhesive Type300

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
DuPont Teijin Films Melinex® ST505 Polyester Film, 500 Gauge
DuPont Teijin Films Melinex® ST505 Polyester Film, 700 Gauge
3M 9472 Adhesive Transfer Tapes with Adhesive 300
3M 9471LE Adhesive Transfer Tapes with Adhesive 300LSE

PMM33232 / 167979

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.