MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Evonik Vestamid® Terra DS 22 natural color Nylon 1010  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: VESTAMID Terra DS22 natural color is a high viscosity PA 1010 basic polymer. VESTAMID Terra DS22 is semi-crystalline, which is the reason for its high mechanical resistance and chemical stability. It absorbs little water so its mechanical properties vary little when exposed to changing environmental humidity. The material features a high dimensional stability. VESTAMID Terra DS22 can be used to manufacture films with good transparency. The high melting point of VESTAMID Terra DS22 compounds results in a high heat deflection temperature. VESTAMID Terra DS22 occupies a position between the high-performance long-chain polyamides such as PA 12 and PA 1212 and shorter chain standard polyamides PA 6 and PA 66. Because of its chemical and physical properties, and the plant origin of its monomers, VESTAMID Terra DS22 is an interesting addition to conventional longer chain polyamides, and it also meets the growing demand for materials made from renewable raw materials. VESTAMID Terra DS22 natural color is supplied as cylindrical granules, ready for processing, in moisture-proof bags. VESTAMID® Terra DS is the polycondensation product of 1,10-decamethylene diamine (D) and 1,10-decanedioic acid (sebacic acid—S). Because both monomers are extracted from castor oil, VESTAMID® Terra DS is based on natural, renewable resources up to 100%.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.05 g/ccISO 1183
Water Absorption at Saturation 1.8 %ISO 62
Viscosity Number 220 cm³/gISO 307
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 54.0 MPaISO 527-1, ISO 527-2
Elongation at Break >= 50 %ISO 527-1, ISO 527-2
Elongation at Yield 5.0 %ISO 527-1, ISO 527-2
Tensile Modulus 1700 MPaISO 527-1, ISO 527-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179-1/1 eU
 NB
@Temperature -30.0 °C
ISO 179-1/1 eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature 23.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 14.0 kJ/m²
@Temperature -30.0 °C
complete break, incl. hinge break H; ISO 179-1/1 eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 200 °C2nd heating, DSC; ISO 11357
Vicat Softening Point 171 °C
@Load 5.10 kg
Method B; ISO 306
 196 °C
@Load 1.02 kg
Method A; ISO 306
 
Descriptive Properties
Global Warming Potential (kgCO2 equivalent/kg material)2.8Evonik, PE International, preliminary data
Renewable Carbon (%)100ASTM 6866

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® RS LC1000 BK385 Nylon 1010
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, dry
AISI 1045 Steel, cold drawn, high temperature, stress relieved, 16-22 mm (0.625-0.875 in) round
DuPont Mobility and Materials Zytel® RS LC1000 BK385 Nylon 1010 (With Extended Stress-Strain Tabular Data)
PTS Trimid® N6-200L Nylon 6 with Lube

PEVONIK987 / 192750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.