MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® RS LC1000 BK385 Nylon 1010
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion

Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight. The material is flexible unreinforced UV and heat sta

Former DuPont product acquired by Celanese in 2022.

Key Words: PA1010
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³DAM; ISO 1183
Moisture Absorption 1.00 %
@Thickness 2.00 mm
1.00 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Viscosity Test 130 cm³/g1.30 dl/gISO 307 1157 1628
Linear Mold Shrinkage, Flow 0.014 cm/cm0.014 in/inDAM; ISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inDAM; ISO 294-4 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 49.0 MPa7110 psi50%RH; ISO 527-1/-2
 60.0 MPa8700 psiDAM; ISO 527-1/-2
Elongation at Break 50 %50 %DAM; Nominal; ISO 527-1/-2
 >= 50 %>= 50 %50%RH; Nominal; ISO 527-1/-2
Elongation at Yield 4.6 %4.6 %DAM; ISO 527-1/-2
 24 %24 %50%RH; ISO 527-1/-2
Tensile Modulus 1.16 GPa168 ksi50%RH; ISO 527-1/-2
 2.10 GPa305 ksiDAM; ISO 527-1/-2
 0.295 GPa
@Temperature 120 °C
42.8 ksi
@Temperature 248 °F
50%RH; ISO 11403-1 -2
 0.311 GPa
@Temperature 120 °C
45.1 ksi
@Temperature 248 °F
DAM; ISO 11403-1 -2
 0.886 GPa
@Temperature 40.0 °C
129 ksi
@Temperature 104 °F
50%RH; ISO 11403-1 -2
 1.249 GPa
@Temperature 40.0 °C
181.2 ksi
@Temperature 104 °F
DAM; ISO 11403-1 -2
 2.388 GPa
@Temperature -40.0 °C
346.4 ksi
@Temperature -40.0 °F
50%RH; ISO 11403-1 -2
 2.407 GPa
@Temperature -40.0 °C
349.1 ksi
@Temperature -40.0 °F
DAM; ISO 11403-1 -2
Flexural Modulus 1.74 GPa252 ksiDAM; ISO 178
Charpy Impact Unnotched NBNBDAM; ISO 179/1eU
 NBNB50%RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50%RH; ISO 179/1eU
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²DAM; ISO 179/1eA
 1.00 J/cm²4.76 ft-lb/in²50%RH; ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
50%RH; ISO 179/1eA
 0.800 J/cm²
@Temperature -30.0 °C
3.81 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 115 µm/m-°C63.9 µin/in-°FDAM; ISO 11359-1/-2
Melting Point 203 °C397 °FDAM; 10°C/min; ISO 11357-1/-3
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
DAM; IEC 60695-11-10
 
Descriptive Properties
Delivery formPellets
Part Marking Code>PA1010<ISO 11469
ProcessingOther Extrusion
 Profile Extrusion
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
Resin IdentificationPA1010ISO 1043
Special characteristicsHeat stabilized or stable to heat
 U.V. stabilized or stable to weather

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Vestamid® Terra DS 22 natural color Nylon 1010
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, dry
DuPont Mobility and Materials Zytel® RS LC1000 BK385 Nylon 1010 (With Extended Stress-Strain Tabular Data)
Suzhou Hipro Polymers Hiprolon® 200 NN Nylon 1010, conditioned
Celanese Zytel® 105F BK010 PA66

PZDSY5479 / 161306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.