MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Advanced Materials PEARLTHANE® 12F75UV Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: PEARLTHANE® D12F75UV is a UV resistant standard polyester based TPU supplied in form of translucent, colorless or slightly yellowish pellets, featuring a low melting point and very low gel content. Processed by extrusion and compounding. PEARLTHANE® D12F75UV is designed for a wide variety of adhesive film applications requiring excellent adhesion in combination with good heat resistance. This grade can be both cast extruded and blown.

All information provided by Merquinsa

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.19 g/cc1.19 g/ccASTM D792
Melt Flow 10 g/10 min
@Load 21.6 kg
10 g/10 min
@Load 47.6 lb
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7878ASTM D2240
Tensile Strength, Yield 30.0 MPa4350 psiASTM D412
Elongation at Break 620 %620 %ASTM D412
100% Modulus 5.00 MPa
@Strain 100 %
725 psi
@Strain 100 %
ASTM D412
300% Modulus 6.50 MPa
@Strain 300 %
943 psi
@Strain 300 %
ASTM D412
Tear Strength 155 kN/m885 pliASTM D624 (Die C)
Abrasion 3535loss (mm³); DIN 53.516
Compression Set  30 %
@Temperature 22.8 °C,
Time 252000 sec
30 %
@Temperature 73.0 °F,
Time 70.0 hour
ASTM D395
 55 %
@Temperature 70.0 °C,
Time 86400 sec
55 %
@Temperature 158 °F,
Time 24.0 hour
ASTM D395
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 - 140 °C266 - 284 °FMQSA 111
Glass Transition Temp, Tg -30.0 °C-22.0 °FDSC, 10ºC/min; DIN 51.007
 
Processing PropertiesMetricEnglishComments
Zone 1 145 - 155 °C293 - 311 °F
Zone 2 155 - 165 °C311 - 329 °F
Zone 3 165 - 175 °C329 - 347 °F
Zone 4 170 - 180 °C338 - 356 °F
Die Temperature 170 - 180 °C338 - 356 °F
Moisture Content <= 0.10 %<= 0.10 %MQSA 44

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Advanced Materials PEARLTHANE® 15N95UV Thermoplastic Polyurethane Elastomer
Covestro DUREFLEX® PT6400 TPU
Lubrizol Advanced Materials PEARLTHANE® 11H98 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlthane® MB-51UV Thermoplastic Polyurethane Elastomer

PMES63 / 88440

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.