MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Adamas Rixon 430 PEEK, 30% Carbon Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:

Information provided by Adamas, HPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.40 - 1.415 g/ccASTM D792
Water Absorption 0.10 - 0.15 %Immersion 24 hrs; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100 - 105ASTM D785
Hardness, Shore D 88 - 90ASTM D2240
Ball Indentation Hardness 410 - 440 MPaISO 2032-N961
Tensile Strength at Break 90.0 - 110 MPaASTM D638
Elongation at Break 5.0 - 7.0 %ASTM D638
Tensile Modulus 1400 - 1450 MPaASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cmASTM D257
Surface Resistance 1e+05ASTM D257
 
Thermal PropertiesOriginal ValueComments
Melting Point 343 °CDSC
Maximum Service Temperature, Air 250 °CDSC
Minimum Service Temperature, Air -80.0 °CDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Tecapeek® XP-114 Compression Molded PEEK Compound, 40% Carbon Fiber
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced
Adamas Rixon 130 PEEK, 30% Carbon Filled

PHADAM002 / 147195

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.