MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm0.00050 - 0.0025 in/in
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  190 MPa
@Temperature 150 °C
27600 psi
@Temperature 302 °F
 215 MPa
@Temperature 120 °C
31200 psi
@Temperature 248 °F
 225 MPa
@Temperature 90.0 °C
32600 psi
@Temperature 194 °F
 235 MPa
@Temperature 60.0 °C
34100 psi
@Temperature 140 °F
 240 MPa
@Temperature 23.0 °C
34800 psi
@Temperature 73.4 °F
Elongation at Break  1.3 %
@Temperature 23.0 °C
1.3 %
@Temperature 73.4 °F
 1.3 %
@Temperature 60.0 °C
1.3 %
@Temperature 140 °F
 1.3 %
@Temperature 90.0 °C
1.3 %
@Temperature 194 °F
 1.4 %
@Temperature 120 °C
1.4 %
@Temperature 248 °F
 1.4 %
@Temperature 150 °C
1.4 %
@Temperature 302 °F
Tensile Modulus  22.6 GPa
@Temperature 150 °C
3280 ksi
@Temperature 302 °F
 23.1 GPa
@Temperature 120 °C
3350 ksi
@Temperature 248 °F
 23.5 GPa
@Temperature 90.0 °C
3410 ksi
@Temperature 194 °F
 23.7 GPa
@Temperature 60.0 °C
3440 ksi
@Temperature 140 °F
 24.0 GPa
@Temperature 23.0 °C
3480 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²
Charpy Impact, Notched 0.500 J/cm²2.38 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 6000 ohm-cm6000 ohm-cm
Surface Resistance 300 ohm300 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 230 °C446 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C>= 572 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °C>= 572 °F
Vicat Softening Point >= 300 °C
@Load 5.00 kg
>= 572 °F
@Load 11.0 lb
 
Processing PropertiesMetricEnglishComments
Melt Temperature 370 - 400 °C698 - 752 °F
Mold Temperature 170 - 200 °C338 - 392 °F
Drying Temperature 120 - 150 °C
@Time 10800 sec
248 - 302 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Adamas Rixon 430 PEEK, 30% Carbon Fiber
Clariant Natural Color Polyethylene Terephthalate Glycol 3D Printer Filament
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced
S-Glass Fiber, Generic
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced

PLATH9642 / 177338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.