MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.41 g/cc
Linear Mold Shrinkage, Flow 0.00050 - 0.0025 cm/cm
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 190 MPa
@Temperature 150 °C
 215 MPa
@Temperature 120 °C
 225 MPa
@Temperature 90.0 °C
 235 MPa
@Temperature 60.0 °C
 240 MPa
@Temperature 23.0 °C
Elongation at Break 1.3 %
@Temperature 23.0 °C
 1.3 %
@Temperature 60.0 °C
 1.3 %
@Temperature 90.0 °C
 1.4 %
@Temperature 120 °C
 1.4 %
@Temperature 150 °C
Tensile Modulus 22600 MPa
@Temperature 150 °C
 23100 MPa
@Temperature 120 °C
 23500 MPa
@Temperature 90.0 °C
 23700 MPa
@Temperature 60.0 °C
 24000 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 40.0 kJ/m²
Charpy Impact, Notched 5.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 6000 ohm-cm
Surface Resistance 300 ohm
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 230 °C
Deflection Temperature at 0.46 MPa (66 psi) >= 300 °C
Deflection Temperature at 1.8 MPa (264 psi) >= 300 °C
Vicat Softening Point >= 300 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 370 - 400 °C
Mold Temperature 170 - 200 °C
Drying Temperature 120 - 150 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Adamas Rixon 430 PEEK, 30% Carbon Fiber
Clariant Natural Color Polyethylene Terephthalate Glycol 3D Printer Filament
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced
S-Glass Fiber, Generic
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced

PLATH9642 / 177338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.