MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Adamas Rixon 430 PEEK, 30% Carbon Fiber
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes:

Information provided by Adamas, HPM

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 - 1.415 g/cc1.40 - 1.415 g/ccASTM D792
Water Absorption 0.10 - 0.15 %0.10 - 0.15 %Immersion 24 hrs; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 100 - 105100 - 105ASTM D785
Hardness, Shore D 88 - 9088 - 90ASTM D2240
Ball Indentation Hardness 410 - 440 MPa59500 - 63800 psiISO 2032-N961
Tensile Strength at Break 90.0 - 110 MPa13100 - 16000 psiASTM D638
Elongation at Break 5.0 - 7.0 %5.0 - 7.0 %ASTM D638
Tensile Modulus 1.40 - 1.45 GPa203 - 210 ksiASTM D638
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cmASTM D257
Surface Resistance 1e+051e+05ASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 343 °C649 °FDSC
Maximum Service Temperature, Air 250 °C482 °FDSC
Minimum Service Temperature, Air -80.0 °C-112 °FDSC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Larpeek 10 K/30 PEEK, 30% Carbon Fiber Reinforced
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Tecapeek® XP-114 Compression Molded PEEK Compound, 40% Carbon Fiber
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced
Adamas Rixon 130 PEEK, 30% Carbon Filled

PHADAM002 / 147195

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.