MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ArcelorMittal Save 30-15 Electrical Steel
Categories: Metal; Ferrous Metal; Alloy Steel

Material Notes: Properties: The iCARe™ Save product family comes with guaranteed losses at 400Hz and indicative maximum values at 700Hz. These values are representative of the steel’s behaviour at high frequencies.

Advantages: Save grades enable you to reduce the iron losses from the stators of synchronous machines. They are particularly useful for reducing iron losses in high-speed hybrid and electric traction machines, and generators which extend the range of electric vehicles.

Applications: Save grades are most effective at reducing iron losses from machine parts which are subject to high base frequencies and additional harmonics. Save thus helps to improve machine efficiency, which leads to an increase in power density. Power density can be tuned to create a lighter, smaller machine, or a more powerful machine for a given weight. Driving range is extended as Save reduces machine weight and costs and saves battery energy.

Recommendations for use: Save grades can be used immediately after lamination punching. The punching effect can be eliminated by performing a stress relief annealing. This optimises their performance in applications with fine teeth, and enables a substantial part of the lower frequency area to be exploited. A C5-type coating is recommended. Save stacks can be produced using existing assembly techniques such as interlocking or welding.

Information provided by ArcelorMittal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.60 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 200 - 230L direction
 200 - 230T direction
Tensile Strength, Ultimate 520 - 560 MPaL direction
 535 - 575 MPaT direction
Tensile Strength, Yield 410 - 450 MPaL direction
 425 - 465 MPaT direction
Elongation at Break 12 - 25 %L direction
 12 - 25 %T direction
 
Magnetic PropertiesOriginal ValueComments
Core Loss <= 15.0 W/kg
@Frequency 400 Hz
at 1T, Guaranteed
 <= 38.0 W/kg
@Frequency 700 Hz
at 1T, Indicative
 
Descriptive Properties
Anisotropy>15%400 Hz at 1T
Polarization>1.49 Tat 2,500 A/m
 >1.6 Tat 5,000 A/m
 >1.7 Tat 10,000 A/m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AK Steel DI-MAX® M-19 Nonoriented Electrical Steel
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive
AK Steel DI-MAX® M-15 Nonoriented Electrical Steel
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel (Extended Electro-Magnetic Data)
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel

NARCE115 / 160023

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.