MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Hytrel® 7246HS BK320 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.018 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.018 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 6515s; ISO 48-4
 <= 71ISO 48-4
Tensile Stress at Strain 23.0 MPa
@Strain 10 %
ISO 527-1/-2
 24.0 MPa
@Strain 50 %
ISO 527-1/-2
Tensile Modulus 510 MPaISO 527-1/-2
Flexural Modulus 510 MPaISO 178
Poissons Ratio 0.47
Tear Strength 165 kN/mnormal; ISO 34-1
 180 kN/mparallel; ISO 34-1
 
Thermal PropertiesOriginal ValueComments
Melting Point 216 °C10°C/min; ISO 11357-1/-3
Brittleness Temperature -68.0 °CISO 974
Glass Transition Temp, Tg 25.0 °C10°C/min; ISO 11357-1/-2
Flame Spread <= 80.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 235 °COptimum, Extrusion
 225 - 245 °CRange, Extrusion
 245 °COptimum, Injection
 235 - 260 °CRange, Injection
Mold Temperature 45.0 °COptimum, Injection
 45.0 - 55.0 °CInjection
Drying Temperature 110 °CInjection
 100 - 120 °CExtrusion
Dry Time 2.00 - 3.00 hourExtrusion, Dehumidified Dryer
 2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.060 %Extrusion
 <= 0.080 %Injection
Hold Pressure <= 70.0 MPaInjection
 
Descriptive Properties
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)280VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Hytrel® 7246 TPC-ET
Celanese Hytrel® 8238 TPC-ET
Celanese Hytrel® 3046 NC010 TPC-ET
Celanese Hytrel® 21UV TPC-ET
Celanese Hytrel® 4556 TPC-ET

PDSX5191 / 197831

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.