MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hytrel® 3046 NC010 TPC-ET
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyester TPE

Material Notes: 30 Shore D High Performance Polyester Elastomer Developed for Injection Molding

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ISO 1183
Moisture Absorption 0.200 %
@Thickness 2.00 mm
0.200 %
@Thickness 0.0787 in
Sim. to ISO 62
Melt Flow 11 g/10 min
@Load 2.16 kg,
Temperature 190 °C
11 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 252515s; ISO 48-4
 <= 30<= 30ISO 48-4
Tensile Stress at Strain  1.90 MPa
@Strain 10 %
276 psi
@Strain 10 %
ISO 527-1/-2
 3.20 MPa
@Strain 50 %
464 psi
@Strain 50 %
ISO 527-1/-2
Izod Impact, Notched (ISO)  NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 180/1A
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact, Notched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
ISO 179/1eA
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
ISO 179/1eA
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 168 °C334 °F10°C/min; ISO 11357-1/-3
Flame Spread 41.0 mm/min
@Thickness 1.00 mm
1.61 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 190 - 210 °C374 - 410 °FRange, Injection
 205 °C401 °FOptimum, Injection
Mold Temperature 30.0 °C86.0 °FOptimum, Injection
 30.0 - 40.0 °C86.0 - 104 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.080 %<= 0.080 %Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)1.5VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Part Marking Code>TPC-ET<ISO 11469
PolymerTPC
Resin IdentificationTPC-ETISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hytrel® 3078 TPC-ET
Celanese Hytrel® 21UV TPC-ET
Celanese Hytrel® 4053FG NC010 TPC-ET
ExxonMobil HD 6480.UV High Density Polyethylene Resin
Celanese Hytrel® 4056 TPC-ET

PDSX5169 / 197809

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.