MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm0.0055 - 0.0075 in/in
Linear Mold Shrinkage, Transverse 0.0065 - 0.0085 cm/cm0.0065 - 0.0085 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break  15.0 MPa
@Temperature 150 °C
2180 psi
@Temperature 302 °F
 20.0 MPa
@Temperature 120 °C
2900 psi
@Temperature 248 °F
 30.0 MPa
@Temperature 90.0 °C
4350 psi
@Temperature 194 °F
 45.0 MPa
@Temperature 60.0 °C
6530 psi
@Temperature 140 °F
 65.0 MPa
@Temperature 23.0 °C
9430 psi
@Temperature 73.4 °F
Elongation at Break  2.5 %
@Temperature 23.0 °C
2.5 %
@Temperature 73.4 °F
 3.5 %
@Temperature 60.0 °C
3.5 %
@Temperature 140 °F
 6.5 %
@Temperature 90.0 °C
6.5 %
@Temperature 194 °F
 12 %
@Temperature 120 °C
12 %
@Temperature 248 °F
 20 %
@Temperature 150 °C
20 %
@Temperature 302 °F
Tensile Modulus  0.500 GPa
@Temperature 150 °C
72.5 ksi
@Temperature 302 °F
 0.750 GPa
@Temperature 120 °C
109 ksi
@Temperature 248 °F
 1.30 GPa
@Temperature 90.0 °C
189 ksi
@Temperature 194 °F
 2.20 GPa
@Temperature 60.0 °C
319 ksi
@Temperature 140 °F
 5.20 GPa
@Temperature 23.0 °C
754 ksi
@Temperature 73.4 °F
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²
Charpy Impact, Notched 0.300 J/cm²1.43 ft-lb/in²
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 550 V550 VA solution
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Deflection Temperature at 0.46 MPa (66 psi) 200 °C392 °F
Deflection Temperature at 1.8 MPa (264 psi) 120 °C248 °F
Vicat Softening Point 205 °C
@Load 5.00 kg
401 °F
@Load 11.0 lb
Flammability, UL94  V-2
@Thickness 3.00 mm
V-2
@Thickness 0.118 in
 V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
Oxygen Index 27 %27 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
1760 °F
@Thickness 0.0394 in
GWFI/GWT
 
Processing PropertiesMetricEnglishComments
Melt Temperature 240 - 260 °C464 - 500 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
194 - 212 °F
@Time 3.00 hour
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
3D Systems DuraForm® ProX® GF Plastic Glass Filled Plastic for SLS® Systems
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized

PLATH9607 / 177303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.