MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems DuraForm® ProX® GF Plastic Glass Filled Plastic for SLS® Systems
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic

Material Notes: Applications: Automotive/under the hood, intake manifolds and other rigid high temperature components, aerospace/aviation, enclosures, cases and covers, power tools and small engine components, jigs and fixtures, thermoforming and hydroforming.

Benefits:

  • Replace molded and CNC-machined glass and mineral-filled plastic articles for short-run production
  • Fuel and oil resistance make it perfect for automotive and aerospace applications
  • Easy to process
Features:
  • Glass-filled composite
  • Best in class rigidity and stiffness
  • Excellent surface finish and resolution
  • Improved thermal resistance versus unfilled materials

Information provided by 3D Systems

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 7373ASTM D 2240
Tensile Strength, Ultimate 45.0 MPa6530 psiASTM D638
Elongation at Break 2.8 %2.8 %ASTM D 638
Tensile Modulus 3.72 GPa540 ksiASTM D 638
Flexural Strength 60.0 MPa8700 psiASTM D 790
Flexural Modulus 3.12 GPa453 ksiASTM D 790
Izod Impact, Notched 0.480 J/cm
@Thickness 3.05 mm
0.899 ft-lb/in
@Thickness 0.120 in
ASTM D 256
Izod Impact, Unnotched 2.07 J/cm
@Thickness 3.05 mm
3.88 ft-lb/in
@Thickness 0.120 in
ASTM D 256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.20e+14 ohm-cm7.20e+14 ohm-cmASTM D257
Surface Resistance 2.76e+14 ohm2.76e+14 ohmASTM D257
Dielectric Constant 3.31
@Frequency 1000 Hz
3.31
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 18.1 kV/mm460 kV/inASTM D149
Dissipation Factor 0.051
@Frequency 1000 Hz
0.051
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  85.3 µm/m-°C
@Temperature 0.000 - 50.0 °C
47.4 µin/in-°F
@Temperature 32.0 - 122 °F
ASTM E 831
 173.7 µm/m-°C
@Temperature 85.0 - 145 °C
96.50 µin/in-°F
@Temperature 185 - 293 °F
ASTM E 831
Specific Heat Capacity 1.26 J/g-°C0.301 BTU/lb-°FASTM E1269
Thermal Conductivity 0.330 W/m-K2.29 BTU-in/hr-ft²-°FASTM E1530
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C264 °FASTM D 648
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems DuraForm® ProX® PA Plastic
3D Systems DuraForm® ProX® HST Composite Thermoplastic Elastomer for SLS® Systems
3D Systems DuraForm® ProX® FR1200 Flame-retardant nylon 12
3D Systems DuraForm® ProX® AF+ Aluminum filled nylon 12 plastic
3D Systems DuraForm® ProX EX BLK Nylon 11 based plastic

PAPPR3110 / 239078

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.