MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

3D Systems DuraForm® ProX® AF+ Aluminum filled nylon 12 plastic
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: DuraForm ProX AF+ is an aluminum filled nylon 12 plastic that produces parts with high stiffness and a metallic appearance

Applications:

  • Housing and enclosures
  • Plastic parts requiring a metallic finish and good appearance
  • Automotive styling parts where a metallic look is needed (knobs, bezzels etc.)
  • High rigidity components
  • Wind tunnel testing parts where stiffness and light weight are needed
Features:
  • Excellent surface finish
  • Easily machined and polished for the addition of press fits, tappings or other uses
  • Repeatable mechanical properties for consistent prints time after time
  • High stiffness for rigid functional assemblies
  • Improved recyclability for an aluminum filled powder
Benefits:
  • Aesthetic metallic surface finish directly off the printer
  • Complex designs can have a metallic look with functional strength at an affordable cost
  • High rigidity ideal for jigs and fixtures
  • Excellent stiffness to weight ratio
  • Lower cost per part due to higher recyclability

Information provided by 3D Systems

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.31 g/cc0.0473 lb/in³Sintered Part; ASTM D792
Water Absorption 0.25 %0.25 %ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 37.0 MPa5370 psiASTM D 638
Elongation at Break 3.0 %3.0 %ASTM D 638
Tensile Modulus 4.34 GPa629 ksiASTM D 638
Flexural Strength 64.0 MPa9280 psiUltimate; ASTM D 790
Flexural Modulus 3.71 GPa538 ksiASTM D 790
Izod Impact, Notched 0.540 J/cm1.01 ft-lb/inASTM D256
Izod Impact, Unnotched 2.55 J/cm4.78 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.09e+14 ohm-cm1.09e+14 ohm-cmASTM D257
Surface Resistance 1.33e+13 ohm1.33e+13 ohmASTM D257
Dielectric Constant 2.6
@Frequency 1000 Hz
2.6
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 3.00 kV/mm76.2 kV/inASTM D149
Dissipation Factor 0.0121
@Frequency 1000 Hz
0.0121
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 145 µm/m-°C
@Temperature 0.000 - 145 °C
80.6 µin/in-°F
@Temperature 32.0 - 293 °F
ASTM E831
Specific Heat Capacity 1.44 J/g-°C0.344 BTU/lb-°FASTM E1269
Thermal Conductivity 0.420 W/m-K2.91 BTU-in/hr-ft²-°FASTM E1530
Deflection Temperature at 0.46 MPa (66 psi) 182 °C360 °FASTM D638
Deflection Temperature at 1.8 MPa (264 psi) 174 °C345 °FASTM D638
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3D Systems DuraForm® ProX® FR1200 Flame-retardant nylon 12
3D Systems DuraForm® ProX® PA Plastic
3D Systems DuraForm® ProX® HST Composite Thermoplastic Elastomer for SLS® Systems
3D Systems DuraForm® ProX® GF Plastic Glass Filled Plastic for SLS® Systems
NRI Syntho-Glass® XT Fiberglass

PAPPR3150 / 239118

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.