MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/cc
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
Linear Mold Shrinkage, Transverse 0.0065 - 0.0085 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 15.0 MPa
@Temperature 150 °C
 20.0 MPa
@Temperature 120 °C
 30.0 MPa
@Temperature 90.0 °C
 45.0 MPa
@Temperature 60.0 °C
 65.0 MPa
@Temperature 23.0 °C
Elongation at Break 2.5 %
@Temperature 23.0 °C
 3.5 %
@Temperature 60.0 °C
 6.5 %
@Temperature 90.0 °C
 12 %
@Temperature 120 °C
 20 %
@Temperature 150 °C
Tensile Modulus 500 MPa
@Temperature 150 °C
 750 MPa
@Temperature 120 °C
 1300 MPa
@Temperature 90.0 °C
 2200 MPa
@Temperature 60.0 °C
 5200 MPa
@Temperature 23.0 °C
Charpy Impact Unnotched 30.0 kJ/m²
Charpy Impact, Notched 3.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 550 VA solution
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 80.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
Vicat Softening Point 205 °C
@Load 5.00 kg
Flammability, UL94 V-2
@Thickness 3.00 mm
 V-2
@Thickness 1.50 mm
 V-2
@Thickness 0.750 mm
Oxygen Index 27 %
Glow Wire Test 960 °C
@Thickness 1.00 mm
GWFI/GWT
 
Processing PropertiesOriginal ValueComments
Melt Temperature 240 - 260 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 90.0 - 100 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
3D Systems DuraForm® ProX® GF Plastic Glass Filled Plastic for SLS® Systems
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled
LATI Kelon® B H CETG/300 PA 6, Glass/Mineral Reinforced, Heat Stabilized
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized

PLATH9607 / 177303

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.