MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Crastin® T835FRUV NC010 PBT  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.43 g/ccISO 1183
Filler Content 5.0 %
Linear Mold Shrinkage 0.013 cm/cm
@Thickness 3.20 mm
Transverse
Linear Mold Shrinkage, Flow 0.014 cm/cm
@Thickness 3.20 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa
@Temperature 23.0 °C
ASTM D638
 62.0 MPa
@Temperature 23.0 °C
ISO 527
Elongation at Break 5.0 %
@Temperature 23.0 °C
ASTM D638
 5.0 %
@Temperature 23.0 °C
ISO 527
Tensile Modulus 3400 MPa
@Temperature 23.0 °C
ISO 527
Flexural Modulus 3100 MPa
@Temperature 23.0 °C
ISO 178
 3200 MPa
@Temperature 23.0 °C
ASTM D790
Izod Impact, Notched 150 J/m
@Temperature 23.0 °C
ASTM D256
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 55.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 120 °CISO 75-1/-2
UL RTI, Electrical 130 °C
@Thickness 0.800 mm
UL 746B
 130 °C
@Thickness 1.50 mm
UL 746B
 130 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical with Impact 130 °C
@Thickness 0.800 mm
UL 746B
 130 °C
@Thickness 1.50 mm
UL 746B
 130 °C
@Thickness 3.00 mm
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 0.800 mm
UL 746B
 130 °C
@Thickness 1.50 mm
UL 746B
 130 °C
@Thickness 3.00 mm
UL 746B
Flammability, UL94 V-0
@Thickness 0.800 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
IEC 60695-11-10
 V-0
@Thickness 3.00 mm
UL94
 V-0
@Thickness 1.50 mm
UL94
 V-0
@Thickness 0.800 mm
UL94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 °COptimum
 240 - 260 °C
Mold Temperature 80.0 °Coptimum
 30.0 - 130 °C
Drying Temperature 110 - 130 °C
Dry Time 2.00 - 4.00 hour
Moisture Content <= 0.040 %
 
Descriptive Properties
AppearanceNatural Color
Drying RecommendedYes
FillerGlass fiber reinforcement
GenericPBT
Material StatusCurrent
Part Marking Code>PBT-IGF5FR(17)<ISO 11469
Polymer FamilyPolyester
Polymer TypePBT
Product CategoryFlame Retardant Resins
 Glass Reinforced Resins
 Toughened Resins
 UV Resistant/Weatherable Resins
Resin IdentificationPBT-IGF5FR(17)ISO 1043

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zytel® ST801AW NC010 PA66-HI
Polyram PlusTek RB703 Nylon 6, UV Stabilized
Celanese Zytel® 105F BK010 PA66
Celanese Zytel® ST801AW BK195 PA66-HI
Celanese Crastin® SK608 BK509 PBT-GF45

PZDSZ1079 / 139896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.