MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Zytel® ST801AW BK195 PA66-HI
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Super Toughened, UV Stabilized, Polyamide 66

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³DAM; ISO 1183
Water Absorption 6.5 %
@Thickness 2.00 mm
6.5 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
 1.1 %
@Thickness 3.00 mm,
Time 86400 sec
1.1 %
@Thickness 0.118 in,
Time 24.0 hour
Immersion; DAM; Sim. to ISO 62
Moisture Absorption 1.90 %
@Thickness 2.00 mm
1.90 %
@Thickness 0.0787 in
DAM; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.018 cm/cm0.018 in/inDAM; ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cm0.014 in/inDAM; ISO 294-4, 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Stress at Strain 41.0 MPa
@Strain 50 %
5950 psi
@Strain 50 %
50% RH; ISO 527-1/-2
Elongation at Break >= 50 %>= 50 %50% RH; ISO 527-1/-2
 75 %75 %50mm/min; DAM; ISO 527-1/-2
Tensile Modulus 1.237 GPa179.4 ksi50% RH; ISO 527-1/-2
 1.90 GPa276 ksiDAM; ISO 527-1/-2
Flexural Modulus 0.700 GPa102 ksi50% RH; ISO 178
 1.80 GPa261 ksiDAM; ISO 178
Poissons Ratio 0.410.41DAM
 0.440.4450% RH
Izod Impact, Notched (ISO)  18.0 kJ/m²
@Temperature -40.0 °C
8.57 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 80.0 kJ/m²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 180/1U
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  1.90 J/cm²
@Temperature -40.0 °C
9.04 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 8.00 J/cm²
@Temperature 23.0 °C
38.1 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 7.40e+12 ohm-cm7.40e+12 ohm-cm50% RH; IEC 62631-3-1
 >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cmDAM; IEC 62631-3-1
Surface Resistance 3.00e+12 ohm3.00e+12 ohm50% RH; IEC 62631-3-2
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
DAM; IEC 62631-2-1
 4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 6.7
@Frequency 100 Hz
6.7
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Dielectric Strength 22.0 kV/mm559 kV/in50% RH; IEC 60243-1
 25.0 kV/mm635 kV/inDAM; IEC 60243-1
Dissipation Factor  0.0060
@Frequency 100 Hz
0.0060
@Frequency 100 Hz
DAM; IEC 62631-2-1
 0.012
@Frequency 1e+6 Hz
0.012
@Frequency 1e+6 Hz
DAM; IEC 62631-2-1
 0.044
@Frequency 1e+6 Hz
0.044
@Frequency 1e+6 Hz
50% RH; IEC 62631-2-1
 0.159
@Frequency 100 Hz
0.159
@Frequency 100 Hz
50% RH; IEC 62631-2-1
Comparative Tracking Index 600 V600 VDAM; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 150 µm/m-°C83.3 µin/in-°FDAM; ISO 11359-1/-2
CTE, linear, Transverse to Flow 130 µm/m-°C72.2 µin/in-°FDAM; ISO 11359-1/-2
Melting Point 262 °C504 °F10°C/min; DAM; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 162 °C324 °FDAM; ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °C144 °FDAM; ISO 75-1/-2
Glass Transition Temp, Tg 20.0 °C68.0 °F10°C/min; 50% RH; ISO 11357-1/-2
 75.0 °C167 °F10°C/min; DAM; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
DAM; IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
DAM; IEC 60695-11-10
Flame Spread 26.0 mm/min
@Thickness 1.00 mm
1.02 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °FOptimum, Extrusion
 275 - 290 °C527 - 554 °FRange, Extrusion
 280 - 300 °C536 - 572 °FRange, Injection
 290 °C554 °FOptimum, Injection
Mold Temperature 50.0 - 100 °C122 - 212 °FInjection
 80.0 °C176 °FOptimum, Injection
Ejection Temperature 190 °C374 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 3.00 - 4.00 hour3.00 - 4.00 hourExtrusion, Dehumidified Dryer
Moisture Content <= 0.060 %<= 0.060 %Extrusion
 <= 0.20 %<= 0.20 %Injection
Hold Pressure 50.0 - 100 MPa7250 - 14500 psiRange, Injection
 
Descriptive Properties
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)38.4VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0.1G-value (condensate); ISO 6452; DAM
ISO designationISO 16396-PA66-I,,M1CG1L1R,S14-020
Max. screw tangential speed (m/s)0.3Injection
Odor Class3VDA 270
Part Marking Code>PA66-HI<ISO 11469
PolymerPA66-I
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPA66-HIISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Zytel® ST801AW NC010 PA66-HI
DuPont Mobility and Materials Zytel® 101L BKB009 PA66
DuPont Mobility and Materials Crastin® T835FRUV NC010 PBT
RTP Company RTP 200 D UV Nylon 6/12 (PA); UV Stabilized
BASF Ultramid® 1000-11 NF2001 PA66 (Dry)

PDSX5513 / 198153

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.